MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC Fluon® FEP 9400 Red Pigmentation
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Fluon® FEP 9400 Series is a full range of color concentrates designed for use in high flow FEP (Fluorinated ethylene propylene) for pigmentation. The color concentrates are based on Teflon® FEP TE-9494 and are supplied in cylindrical pellet form. These pellets are approximately 0.080” long by 0.080” diameter.

End Uses: Colored injection molded parts, film, tubing, colored wire or jacket insulation where a pigmented appearance is required.

Information provided by AGC Chemicals Americas Inc.

Key Words: 428-015-406
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 1.20 g/cc
Melt Flow 22 g/10 min
ASTM Color 33.8b, CIELAB, 10° obs., D65
 41.2L, CIELAB, 10° obs., D65
 54.5a, CIELAB, 10° obs., D65
 3020RAL
 
Descriptive Properties
Dispersion Quality0.0015 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Fluorinated Ethylene Propylene (FEP), Molded/Extruded
AGC Fluon® FEP 100 Red Pigmentation
Samyang Trirex® 3027A Polycarbonate
Chemours 100 FEP Fluorinated Ethylene Propylene

PAGCX187 / 191296

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.