MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AGC Fluon® FC100-25 1000 PTFE, 25% Glass Fiber Filled
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes:

Information provided by AGC Chemicals Americas Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.25 g/cc
Filler Content 22.2 %by volume
 25 %by weight
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 5570
Tensile Strength 1000 - 1600 psiExtruded
 1800 - 2800 psiMolded
Tensile Stress at Strain 6.00 kg(f)/cm²
@Strain 1 %,
Temperature 250 °C
 8.00 kg(f)/cm²
@Strain 1 %,
Temperature 220 °C
 10.0 kg(f)/cm²
@Strain 1 %,
Temperature 180 °C
 11.0 kg(f)/cm²
@Strain 2 %,
Temperature 250 °C
 15.0 kg(f)/cm²
@Strain 2 %,
Temperature 220 °C
 17.0 kg(f)/cm²
@Strain 3 %,
Temperature 250 °C
 17.0 kg(f)/cm²
@Strain 1 %,
Temperature 140 °C
 20.0 kg(f)/cm²
@Strain 2 %,
Temperature 180 °C
 22.0 kg(f)/cm²
@Strain 4 %,
Temperature 250 °C
 22.0 kg(f)/cm²
@Strain 3 %,
Temperature 220 °C
 27.0 kg(f)/cm²
@Strain 1 %,
Temperature 100 °C
 28.0 kg(f)/cm²
@Strain 4 %,
Temperature 220 °C
 28.0 kg(f)/cm²
@Strain 3 %,
Temperature 180 °C
 32.0 kg(f)/cm²
@Strain 2 %,
Temperature 140 °C
 36.0 kg(f)/cm²
@Strain 4 %,
Temperature 180 °C
 37.0 kg(f)/cm²
@Strain 1 %,
Temperature 60.0 °C
 43.0 kg(f)/cm²
@Strain 3 %,
Temperature 140 °C
 47.0 kg(f)/cm²
@Strain 2 %,
Temperature 100 °C
 53.0 kg(f)/cm²
@Strain 4 %,
Temperature 140 °C
 60.0 kg(f)/cm²
@Strain 2 %,
Temperature 60.0 °C
 61.0 kg(f)/cm²
@Strain 3 %,
Temperature 100 °C
 63.0 kg(f)/cm²
@Strain 1 %,
Temperature 20.0 °C
 71.0 kg(f)/cm²
@Strain 4 %,
Temperature 100 °C
 75.0 kg(f)/cm²
@Strain 3 %,
Temperature 60.0 °C
 86.0 kg(f)/cm²
@Strain 4 %,
Temperature 60.0 °C
 >= 89.0 kg(f)/cm²
@Strain 4 %,
Temperature 20.0 °C
 >= 89.0 kg(f)/cm²
@Strain 3 %,
Temperature 20.0 °C
 89.0 kg(f)/cm²
@Strain 2 %,
Temperature 20.0 °C
Elongation at Break 100 - 200 %Extruded
 200 - 300 %Molded
Coefficient of Friction, Dynamic 0.11
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 2.00e+15 ohm-cm
Surface Resistance 1.00e+15 ohmAmbient humidity
 1.00e+15 ohm95% RH
Dielectric Constant 2.2 - 2.5
@Frequency 100000 - 1.00e+7 Hz
Ambient humidity
 2.2 - 2.5
@Frequency 100000 - 1.00e+7 Hz
95% RH
Dielectric Loss Index 0.00097
@Frequency 10000 Hz
dry
 0.0017
@Frequency 1000 Hz
dry
 0.062
@Frequency 1e+6 Hz
after 9 weeks at 95% RH
 0.225
@Frequency 100000 Hz
after 9 weeks at 95% RH
 0.28
@Frequency 10000 Hz
after 9 weeks at 95% RH
 0.39
@Frequency 1000 Hz
after 9 weeks at 95% RH
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 67.14 µm/m-°C
@Temperature 30.0 - 250 °C
 67.69 µm/m-°C
@Temperature 30.0 - 200 °C
 68.17 µm/m-°C
@Temperature 30.0 - 150 °C
 68.59 µm/m-°C
@Temperature 30.0 - 100 °C
 68.72 µm/m-°C
@Temperature 15.0 - 30.0 °C
 68.86 µm/m-°C
@Temperature 30.0 - 50.0 °C
 69.0 µm/m-°C
@Temperature -60.0 - 15.0 °C
CTE, linear, Transverse to Flow 62.46 µm/m-°C
@Temperature 30.0 - 250 °C
 63.04 µm/m-°C
@Temperature 30.0 - 200 °C
 63.36 µm/m-°C
@Temperature 30.0 - 150 °C
 63.68 µm/m-°C
@Temperature 30.0 - 100 °C
 63.87 µm/m-°C
@Temperature 15.0 - 30.0 °C
 63.87 µm/m-°C
@Temperature 30.0 - 50.0 °C
 64.0 µm/m-°C
@Temperature -60.0 - 15.0 °C
Thermal Conductivity 2.60 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C
Minimum Service Temperature, Air -250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AGC Fluon® FC168-63 PTFE, 63% Bronze and Graphite Filled
AGC Fluon® RB1025S 25% Glass Fiber, PTFE Filled Compound
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
Hippe PTFE

PAGCX289 / 191398

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.