MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced; Rubber or Thermoset Elastomer (TSE)

Material Notes: MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outstanding hydrolytic stability and improved processing. MILLATHANE E34 can be compounded and processed by the use of conventional rubber manufacturing equipment — mixed on two roll mills or an internal mixer. Compounds can be — calendered; extruded; injection, transfer, or compression molded — to produce finished polyurethane parts. It can be vulcanized by organic peroxides or sulfur with thiazole accelerators.

All information provided by TSE Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/cc
Mooney Viscosity  35 - 65
@Temperature 100 °C
35 - 65
@Temperature 212 °F
ML 1+4
 40 - 60
@Temperature 100 °C
40 - 60
@Temperature 212 °F
Standard, ML 1+4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 45 - 9045 - 90
Tensile Strength 40.0 MPa5800 psi
Resilience 40 - 5040 - 50
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -62.0 °C-79.6 °F
 
Descriptive Properties
AppearancePale to dark amber solid bale or milled sheets
Health HazardNone
Hydrolytic StabilityVery Good
OdorFaint, characteristic
Oil and Fuel ResistanceVery Good
Ozone ResistanceExcellent
Storage StabilityExcellent
Weather ResistanceVery Good

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
C.O.I.M. LARIPUR® LPR2103-90AE PTMG Polyether Polyurethane
Huntsman IROGRAN® A 95 P 5044 DP TPU-Polyether
C.O.I.M. LARIPUR® LPR70D60 PTMG Polyether Polyurethane
Dow PELLETHANE® 2101-85A Polyurethane Elastomer (Ether-Ether Hybrid)
Dow Pellethane® 2103-90AEF Polyurethane Elastomer, Ether Based

PMILL383 / 87427

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.