MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Avient Dynalloy™ 8900-30 Thermoplastic Elastomer (TPE)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Dynalloy™ 8900-series is an innovative thermoplastic elastomer selection formulated to provide the injection molder with a product capable of overmolding and bonding to both low-density polyethylene (LDPE) and polypropylene (PP) with efficient cycle times. - Adhesion to Low-Density Polyethylene and Polypropylene - Flexible - Colorable

Color concentrates with polypropylene (PP), ethylene vinyl acetate (EVA), or low density polyethylene (PE) carriers are most suitable for coloring Dynalloy™ 8900-series. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow from 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. Concentrates based on PVC should not be used. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polyethylene (PE) or polypropylene (PP). The Dynalloy™ 8900-series has excellent melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 8 - 10 minutes or longer. Drying is not Required Injection Speed: 1 to 3 in/sec 1st Stage - Boost Pressure: 175 to 800 psi 2nd Stage - Hold Pressure: 30% of Boost Hold Time (Thick Part): 3 to 10 sec Hold Time (Thin Part): 1 to 3 sec

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.878 g/ccASTM D792
Viscosity 6700 cP
@Shear Rate 11200 1/s,
Temperature 200 °C
ASTM D3835
 27000 cP
@Shear Rate 1340 1/s,
Temperature 200 °C
ASTM D3835
Linear Mold Shrinkage, Flow 0.0090 - 0.014 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 3010 sec; ASTM D2240
Tensile Strength at Break 2.07 MPa
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tensile Stress at Strain 1.03 MPa
@Strain 100 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
 1.55 MPa
@Strain 300 %,
Temperature 23.0 °C
Die C2 hr; ASTM D412
Elongation at Break 800 %
@Temperature 23.0 °C
Die C2 hr; ASTM D412
Tear Strength 14.0 kN/mASTM D624
Compression Set 17 %
@Temperature 23.0 °C,
Time 79200 sec
25% deflection; ASTM D395B
 40 %
@Temperature 70.0 °C,
Time 79200 sec
25% deflection; ASTM D395B
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 160 - 182 °C
Middle Barrel Temperature 171 - 193 °C
Front Barrel Temperature 182 - 204 °C
Nozzle Temperature 182 - 204 °C
Mold Temperature 15.6 - 26.7 °C
Back Pressure 0.000 - 0.689 MPa
Screw Speed 25 - 100 rpm
 
Compliance PropertiesOriginal ValueComments
FDA Yes21 CFR 177.1210
 
Descriptive Properties
Agency RatingsBfR XXI, section 2.1.3.1.1
AppearanceNatural Color
FeaturesGood Colorability
 Good Processability
 Good Processing Stability
 High Flow
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodInjection Molding
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
RoHS ComplianceRoHS Compliant
UsesConsumer Applications
 Flexible Grips
 General Purpose
 Household Goods
 Non-specific Food Applications
 Overmolding
 Soft Touch Applications
 Sporting Goods
 Thin-walled Parts

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Dynalloy™ OBC8000-T60 Thermoplastic Elastomer (TPE)
Avient Dynaflex™ G7930-1001-00 Thermoplastic Elastomer (TPE)
Avient Dynalloy™ 8900-80 Thermoplastic Elastomer (TPE)
Avient Versaflex™ OM 1245X-1 Thermoplastic Elastomer (TPE)
Avient Versalloy™ XL 9055X-9 Thermoplastic Elastomer (TPE)

PH0POL1094 / 145663

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.