MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ IM 401-11 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: CALIBRE™ IM 401-11 Impact Modified Polycarbonate resin is available in opaque formulations that offer benefits ranging from superior low temperature impact strength to easy processing with improved impact strength in highly filled formulations

Main Characteristics:

  • Impact modified
  • Superior low temperature toughness
Applications:
  • Automotive interiors
  • Automotive exteriors
  • Small & large applications
Automotive Specifications:
  • FORD WSS-M4D100-C1
  • GM GMP.PC.003

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183/B
Linear Mold Shrinkage, Flow 0.0060 - 0.0080 in/inISO 294-4
Melt Flow 11 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 55.8 MPa50 mm/min; ASTM D638
 56.0 MPaISO 527-2/50
Elongation at Break 130 %50 mm/min; ASTM D638
 130 %ISO 527-2/50
Flexural Strength 89.6 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
 90.0 MPa2.0 mm/min, 3 points; ISO 178
Flexural Modulus 2270 MPa2.0 mm/min, 3 points; ISO 178
 2280 MPaMethod I (3 point load), 2.0 mm/min; ASTM D790
Izod Impact, Notched 690 J/mASTM D256
Tensile Impact Strength 630 kJ/m²ASTM D1822
Dart Drop, Total Energy 56.5 J3.39 m/sec; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 121 °CUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 136 °CAnnealed; ISO 75-2/A
Vicat Softening Point 146 °CISO 306/B50
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ravago Manufacturing Americas Hylex® P1310G20 HB Polycarbonate, 20% Fiberglass Reinforced, UV Stabilized
Ravago Manufacturing Americas Hylex® P1310G10 HB Polycarbonate, 10% Fiberglass Reinforced, UV Stabilized
SABIC Lexan® 121 PC
Trinseo CALIBRE™ 200-23 Polycarbonate Resin
Mocom (ALBIS) ALTECH® PC-HT A 1000/500 High Heat Polycarbonate

PDWST007 / 142216

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.