MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis LE1120 Low Density Polyethylene for Physically Foamed Cellular Insulation  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Wire/Cable Grade

Material Notes: LE1120 is a low density polyethylene intended for the insulation of coaxial and radio frequency communication cables.. It contains no additives and is designed to give the lowest possible attenuation by the selection of "electrically clean" feedstock. Strict cleanliness requirements are applied in production and materials handling.

LE1120 is designed to be used as insulation for radio frequency cables having extra high demand on low attenuation at high frequencies. By blending weight a suitable stabilized HDPE component prior to the extrusion, in an optimum ratio for each insulation thickness, the lowest possible attenuation can be achieved. A small amount of HE1102 is recommended as nucleating agent. Using optimized-processing conditions an expansion above 80% can be expected.

Former trade name for this product was Borcell™.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccISO 1183
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 45ISO 868
Tensile Strength, Yield 1769 psiISO 527-2
Elongation at Break 500 %ASTM D638
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.28
@Frequency 1.80e+9 Hz
Borealis Test
 2.29
@Frequency 3.90e+9 Hz
Borealis Test
 2.3
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.000040
@Frequency 1e+6 Hz
IEC 60250
 0.00015
@Frequency 1.80e+9 Hz
Borealis Test
 0.00017
@Frequency 3.90e+9 Hz
Borealis Test
 
Processing PropertiesOriginal ValueComments
Middle Barrel Temperature >= 180 °C
Front Barrel Temperature >= 150 °C
Die Temperature >= 365 °F
Head Temperature >= 185 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HE1344 High Density Polyethylene Compound for Cellular Insulation of Data Cables
Borealis HE1345 High Density Polyethylene Compound for Cellular Insulation of Telephone Singles
Borealis Borcell™ HE1102 High Density Polyethylene Compound for Gas Injection of Cellular Communication Cable Insulation
Borealis WE150CF PO Compound for Sterilizable Peelable Film Applications
Borealis HE4873 High Density Polyethylene

PBOREA030 / 27337

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.