MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel; T S30000 Series Stainless Steel

Material Notes: CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized corrosion. The grade is stabilized by the addition of Titanium that avoids intergranular corrosion and ensures good mechanical properties at room and elevated temperature. Alloy CLC 17-12-2Ti is an austenitic microstructure grade, free of deleterious carbide precipitations but containing CNTi precipitations on grain boundaries. The grain is regularly fine and contains some residual ferrite (approx 4%) after solution annealing (1050-1150°C – 1922-2102°F) and water quenching. The CLC 17-12-2Ti steel resists much better to wet atmosphere or solution containing chloride or fluoride addition. The steel is not seawater resistant. The alloy may be used in diluted chloridric or sulphuric acids at low temperature (= 330°C - 626°F) as well as in sour organic solutions. The grade is also well known for its high ductility, particularly when considering cold forming.

Information provided by manufacturer.

Key Words: EURONORM 1.4571 X6CrNiMo 17.12.2, AFNOR Z6 CNDT 17-12, DIN W1.4571, ASTM A 240 TP 316Ti, UNS S31635
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 560 MPaTypical
 520 - 670 MPaMinimum Guaranteed
Tensile Strength, Yield >= 220 MPa
@Strain 0.2 %
 >= 260 MPa
@Strain 1 %
 270 MPa
@Strain 0.2 %
Typical
 310 MPa
@Strain 1 %
Typical
Elongation at Break 40 - 60 %
Creep Strength 250 MPa
@Temperature 600 °C,
Time 3.60e+6 sec
Modulus of Elasticity 200 GPa
@Temperature 20.0 - 100 °C
Poissons Ratio 0.299Calculated
Shear Modulus 77.0 GPa
@Temperature 20.0 - 100 °C
Charpy Impact >= 125 J
 225 JTypical
 >= 100 J
@Temperature -196 °C
 188 J
@Temperature -196 °C
Typical
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000750 ohm-cm
@Temperature 20.0 - 100 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 20.0 - 100 °C
 17.5 µm/m-°C
@Temperature 20.0 - 200 °C
 18.0 µm/m-°C
@Temperature 20.0 - 300 °C
 19.0 µm/m-°C
@Temperature 20.0 - 500 °C
Specific Heat Capacity 0.500 J/g-°C
@Temperature 20.0 - 100 °C
Thermal Conductivity 15.0 W/m-K
@Temperature 20.0 - 100 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.050 %
Chromium, Cr 17 %
Iron, Fe 71.25 - 71.7 %As remainder
Molybdenum, Mo 2.1 %
Nickel, Ni 11 %
Titanium, Ti 0.25 - 0.70 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
316 Stainless Steel, annealed bar
Crucible Steel 431 Chromium Steel
Schmolz + Bickenbach UGICHROM 4057 Martensitic Chrome Plated Bar
Kinetics MIM 17-4PH Stainless Steel (H1100 Condition)

NINDUST07 / 17545

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.