MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lanxess Adimoll® BO Plastic Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Adimoll® BO is a low-temperature-resistant plasticizer suitable for a large number of polymers, inclusive polyvinyl chloride (PVC), rubbers, nitro- and ethyl cellulose, and polyvinyl acetate (PVAC).

Chemical composition: Benzyl octyl adipate (BOA)

CAS reg. no.: 58394-64-2

General Adimoll® BO is characterized by

  • a very good plasticizing effect when used with PVC, PVAC, NBR and other polymers.
  • a low viscosity, which, in combination with its weak ability to solvate PVC, has a positive effect on the initial viscosity and storage stability of plastisols.
  • a good compatibility with a large number of polymers.
Adimoll® BO imparts
  • very good low-temperature resistance to suitably plasticized compounds; this effect is clearly noticeable even when Adimoll® BO is used in combination with other plasticizers.
  • very good rebound resilience to PVC and PVC / NBR blends.
  • very good light stability to PVC compounds.
Applications: Adimoll® BO is used for a wide range of articles based on polyvinyl chloride (PVC), acrylonitrile butadiene rubber (NBR), styrene-butadiene rubber (SBR), chloroprene rubber (CR), ethylene-vinyl acetate rubber (EVM) and ethylene-propylene copolymers (EPM). Adimoll® BO is also compatible with nitro- and ethyl cellulose, polystyrene and natural rubber. It has a limited compatibility with cellulose acetate butyrate and cellulose propionate. It is particularly beneficial to use Adimoll® BO when very good low-temperature resistance and light stability are required, together with high elasticity. Typical fields of applications are coatings (including spreading), calendering, extrusion, injection molding and adhesive industry.

Information provided by Lanxess.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccDIN 53 015
Water Absorption <= 0.10 %DIN 51 777
Viscosity 16 cP
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.10[mg KOH/g]; DIN EN ISO 2114
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.48DIN EN ISO 6320
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Descriptive Properties
Color<80Hazen, ISO 6271
Specifications131°CDissolution temperature, DIN 53408

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 8863 Moldings & Extrusions Flexible PVC
Colorite Polymers 2019F Rigid PVC
Teknor Apex Sinvicomp SFE 5000 Polyvinyl Chloride, Flexible
Iran Petrochemical (PCC) PVC-S7054 Poly Vinyl Chloride
Geon® Performance Solutions Vinyl Flexible XV3645 Polyvinyl Chloride, Flexible

PLANY8234 / 208627

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.