MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilon® BFZ 3 PA6
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6)

Material Notes: Product description: Grilon BFZ 3 is an unreinforced, high impact resistant PA6 extrusion grade. Grilon BFZ 3 has the following important properties:
  • Extreme toughness
  • Easy processing
  • Low density
Grilon BFZ 3 is used in coextrusion as a barrier layer and to improve the mechanical properties of blow molded parts.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccDry; ISO 1183
Water Absorption 9.0 %Sim. to ISO 62
Moisture Absorption 3.00 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.014 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 40.0 MPaConditioned; ISO 2039-1
 95.0 MPaDry; ISO 2039-1
Tensile Strength, Yield 25.0 MPaConditioned; ISO 527-1/-2
 50.0 MPaDry; ISO 527-1/-2
Elongation at Break >= 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 4.0 %Dry; ISO 527-1/-2
 15 %Conditioned; ISO 527-1/-2
Tensile Modulus 600 MPaConditioned; ISO 527-1/-2
 1800 MPaDry; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
Dry; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
Dry; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 65.0 kJ/m²
@Temperature 23.0 °C
Dry; ISO 179/1eA
 115 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+10 ohm-cmConditioned; IEC 60093
 1.00e+12 ohm-cmDry; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 39.0 kV/mmConditioned; IEC 60243-1
 42.0 kV/mmDry; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 130 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 150 µm/m-°CISO 11359-1/-2
Melting Point 222 °C10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 - 110 °CLong Term; ISO 2578
 160 °CShort Term; EMS
Deflection Temperature at 0.46 MPa (66 psi) 130 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Compliance PropertiesOriginal ValueComments
FDA YesFood contact
 
Descriptive Properties
Electricals & ElectronicsCables & Tubes
Food contactEU Requirements
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Power transmission
 Tools & Accessories
PackagingBlow molded containers
 Injection, stretch, blow molded containers
ProcessingExtrusion - blow molding
 Injection Molding
 Other Extrusion
Product AttributesBarrier Properties
 Flexible
Special CharacteristicsHigh impact or impact modified

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Polyetheretherketone, Unreinforced
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced
Overview of materials for Polycarbonate, 30% Glass Filled
Overview of materials for Polyphenylene Sulfide (PPS); Molded
EMS-Grivory Grilamid® XE 4181 nat PA1010

PGRH162 / 156871

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.