MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Aluminum 2219-T6
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN.

Composition Notes: Composition information provided by the Aluminum Association and is not for design.

Key Words: UNS A92219; Aluminium 2219-T6; AA2219-T6; Al2219-T6
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.84 g/ccAA; Typical
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate >= 365 MPaHand forgings; Short transverse axis
 >= 365 MPaRolled rings; Radial axis
 >= 380 MPaHand forgings; Long transverse axis
 >= 380 MPaRolled rings; Axial axis
 >= 385 MPaDie forgings; Specimen axis not parallel to grain flow
 >= 385 MPaRolled rings; Tangential axis
 >= 400 MPaDie forgings; Specimen axis parallel to grain flow
 >= 400 MPaHand forgings; Longitudinal
Tensile Strength, Yield >= 240 MPaHand forgings; Short transverse axis
 >= 240 MPaRolled rings; Radial axis
 >= 250 MPaDie forgings; Specimen axis not parallel to grain flow
 >= 255 MPaHand forgings; Long transverse axis
 >= 255 MPaRolled rings; Axial axis
 >= 260 MPaDie forgings; Specimen axis parallel to grain flow
 >= 275 MPaHand forgings; Longitudinal
 >= 275 MPaRolled rings; Tangential axis
Elongation at Break 2.0 %Hand forgings; Short transverse axis
 2.0 %Rolled rings; Radial axis
 4.0 %Die forgings; Specimen axis not parallel to grain flow
 4.0 %Hand forgings; Long transverse axis
 4.0 %Rolled rings; Axial axis
 6.0 %Hand forgings; Longitudinal
 6.0 %Rolled rings; Tangential axis
 8.0 %Die forgings; Specimen axis parallel to grain flow
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 35.0 ohm-cir-mil/ft
@Temperature 20.0 °C
AA; Typical
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.4 µin/in-°F
@Temperature 20.0 - 100 °C
AA; Typical; average over range
 20.8 µm/m-°C
@Temperature -50.0 - 20.0 °C
 22.5 µm/m-°C
@Temperature 20.0 - 100 °C
 23.4 µm/m-°C
@Temperature 20.0 - 200 °C
 24.4 µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity 840 BTU-in/hr-ft²-°FAA; Typical at 77°F
Melting Point 1010 - 1190 °FAA; Typical range based on typical composition for wrought products >= 1/4 in. thickness. Eutectic melting is not eliminated by homogenization.
Solidus 1010 °FAA; Typical
Liquidus 1190 °FAA; Typical
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 775 °F
Solution Temperature 995 °F
Aging Temperature 325 - 375 °Ffrom 18 to 36 hr at temperature
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al 91.5 - 93.8 %As remainder
Copper, Cu 5.8 - 6.8 %
Iron, Fe <= 0.30 %
Magnesium, Mg <= 0.02 %
Manganese, Mn 0.20 - 0.40 %
Other, each <= 0.05 %
Other, total <= 0.15 %
Silicon, Si <= 0.20 %
Titanium, Ti 0.02 - 0.10 %
Vanadium, V 0.05 - 0.15 %
Zinc, Zn <= 0.10 %
Zirconium, Zr 0.10 - 0.25 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aluminum 2319
2519 Aluminum Composition Spec
Aluminum 2219-O
Aluminum 2219-T62
Aluminum 2014-T6; 2014-T651

MA2219T6 / 8931

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.