MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teijin Multilon TN-7500 Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has excellently high flowability, i.e., suitable for a large-scale business machine chassis.

Information provided by Teijin Chemicals Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.18 g/ccISO 1183
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm
@Thickness 4.00 mm
Linear Mold Shrinkage, Transverse 0.0040 - 0.0060 cm/cm
@Thickness 4.00 mm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 47.0 MPa50mm/min; ISO 527
Tensile Strength, Yield 63.0 MPa50mm/min; ISO 527
Elongation at Break 50 %50mm/min; ISO 527
Elongation at Yield 3.0 %50mm/min; ISO 527
Flexural Strength 95.0 MPa2mm/min; ISO 178
Flexural Modulus 2.60 GPa2mm/min; ISO 178
Charpy Impact Unnotched NBISO 179
Charpy Impact, Notched 1.30 J/cm²ISO 179
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 20.0 °C
ISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °CISO 75
Flammability, UL94 V-0
@Thickness 1.50 mm
 5VA
@Thickness 2.00 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teijin Multilon TN-7500F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Teijin Multilon TN-7000 Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Teijin Multilon TN-7100F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Teijin Panlite® LN-2250Y Flame Resistant, Translucent Polycarbonate Resin
Teijin Multilon DN-1520B Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy

PTEIJ46 / 69735

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.