MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Bynel® 21E533 Anhydride Modified Ethylene Acrylate
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: BYNEL® Series 2100 resins are anhydride modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins.

BYNEL 21E533 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlayers in composite packages for food use. This regulation describes adhesives which may be safely used as components of articles intended for use in packaging, transporting or holding food. This regulation requires that either (1) the adhesive is separated from the food by a functional barrier, or (2) the quantity of adhesive which contacts fatty or aqueous foods does not exceed the trace amounts at the seams or edges.

This former DuPont product line is now a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccASTM D792, ISO 1183
Melt Flow 7.7 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Thermal PropertiesOriginal ValueComments
Melting Point 64.0 °CFreezing Point; ASTM D3418
 83.0 °CASTM D3418, ISO 3146
Vicat Softening Point 50.0 °CASTM D1525, ISO 306
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 260 °C
Feed Temperature 135 °CCoExtrusion with EVOH Processing
 135 °CCoExtrusion with Nylon Processing
Zone 2 185 °CCoExtrusion with EVOH Processing
 185 °CCoExtrusion with Nylon Processing
Zone 3 210 °CCoExtrusion with EVOH Processing
 235 °CCoExtrusion with Nylon Processing
Zone 4 235 °CCoExtrusion with EVOH Processing
 260 °CCoExtrusion with Nylon Processing
Zone 5 235 °CCoExtrusion with EVOH Processing
 260 °CCoExtrusion with Nylon Processing
Adapter Temperature 235 °CCoExtrusion with EVOH Processing
 260 °CCoExtrusion with Nylon Processing
Die Temperature 235 °CCoExtrusion with EVOH Processing
 260 °CCoExtrusion with Nylon Processing
Melt Temperature 210 - 235 °CCoExtrusion with EVOH Processing
 <= 260 °CCoExtrusion with Nylon Processing

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow Bynel® 22E757 Modified Ethylene Acrylate
Dow Bynel® 2022 Acid-Modified Ethylene Terpolymer Adhesive Resin
Dow Bynel® 2002 Acid-Modified Ethylene Terpolymer Adhesive Resin
Dow Bynel® 21E810 Anhydride Modified Ethylene Acrylate
Dow Bynel® 21E830 Anhydride Modified Ethylene Acrylate

PDTA4912 / 170352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.