MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CeramTec SL 200 BG Silicon Nitride, Si3N4-Y2O3
Categories: Ceramic; Nitride

Material Notes: SL 200 BG is a silicon nitride ceramic used to make welding rollers, pins, and components, gas nozzles, and forming tools. Silicon nitrides are ideal for components working under mechanical loads and engine parts, even and especially at elevated temperatures. Their property profile includes: extremely high strength, good crack resistance, outstanding wear resistance, good heat conductivity, very low heat expansion, and good resistance to sudden changes in temperature. Due to these properties and its low weight, silicon nitride is a material for the highest demands.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.21 g/cc0.116 lb/in³DIN EN 623-2
Water Absorption 0.00 %0.00 %Open Porosity; DIN EN 623-2
Permeability 0.000.00%, Gas
Weibull Modulus 1616DINV ENV 843-5
 
Mechanical PropertiesMetricEnglishComments
Vickers Microhardness 16501650HV1; DINV ENV 843-4
Tensile Modulus 310 GPa45000 ksiYoung's; DINV ENV 843-2
Flexural Strength 850 MPa123000 psiDIN EN 843-1
Compressive Strength 3000 MPa435000 psiDIN 51067T1
Poissons Ratio 0.260.26DINV ENV 843-2
Fracture Toughness 7.00 MPa-m½6.37 ksi-in½KIC (SEVNB); DIN CEN/TS 14425-1
Shear Modulus 123 GPa17800 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 672-1
Dielectric Constant 8.0
@Frequency 1e+6 Hz
8.0
@Frequency 1e+6 Hz
IEC 672-1
Dielectric Strength 19.0 kV/mm483 kV/inIEC 672-1
Dielectric Loss Index 0.0040
@Frequency 1e+9 Hz
0.0040
@Frequency 1e+9 Hz
IEC 672-1
 
Thermal PropertiesMetricEnglishComments
CTE, linear  3.20 µm/m-°C
@Temperature 20.0 - 400 °C
1.78 µin/in-°F
@Temperature 68.0 - 752 °F
DIN EN 821-1
 4.30 µm/m-°C
@Temperature 20.0 - 1000 °C
2.39 µin/in-°F
@Temperature 68.0 - 1830 °F
DIN EN 821-1
Specific Heat Capacity 0.700 J/g-°C0.167 BTU/lb-°FDINV ENV 821-3
Thermal Conductivity 21.0 W/m-K146 BTU-in/hr-ft²-°FDIN EN 821-2
Maximum Service Temperature, Air 1300 °C2370 °F
Maximum Service Temperature, Inert 1600 °C2910 °F
 
Descriptive Properties
Ra = Arithmetic Mean Roughness Value (µm)<0.1
Thermal Shock Resistance R1 (K)569calculated; R1 = [σs (1-µ)] / (α·E)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Silicon Nitride, reaction sintered
CeramTec SL 200 ST Silicon Nitride, Si3N4-Y2O3
3M Techical Ceramics Ekasic® S Silicon Nitride
Silicon Nitride
Silicon Nitride, Si3N4

CCERA916 / 107516

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.