MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Teknor Apex Sinpolene MBN7541 Linear Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Sinpolene MBN7541 is an additive concentrate which contains processing aid to eliminate or deuce melt fracture and die build-up during processing of LLDPE and HDPE. Also effective in increasing throughput and reducing power consumption.

Availability: Africa & Middle East; Asia Pacific; Latin America

Additive: Processing Aid: 3%

Features: Low Odor

Uses: Profiles; Sheet

Form: Pellets

Processing Method: Injection Molding; Profile Extrusion; Sheet Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 3.0 - 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Teknor Apex Sinpolene MBN7574 Polypropylene
Struktol TR 131 Slip Agent, Lubricant, Mold Release Agent
LyondellBasell Hostacom ERC 204N NAT Polypropylene with 10% Talc Filler
Evonik TEGO® Sorb PY 88 TQ Odour absorber
Abatron ClearStrip™ Stripper for Paint, Varnish, Coatings; Gel

PTEKNQ1339 / 237830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.