MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPH 3622 Polypropylene, Injection Molding Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: General purpose injection molding and extrusion homopolymer

Good Processability -- FINA 3622 is engineered for good processability in thin wall multi- cavity molds.

Good Clarity -- FINA 3622 has good contact/see-through clarity, and is easily printed with silk screen or hot stamping techniques.

FDA -- FINA 3622 complies with all applicable FDA regulations and may be used under those provisions for food contact applications.

Recommended Applications-- FINA 3622 is recommended for the injection molding of housewares, utility boxes, and containers, as well as, general purpose extrusion.

Processing -- FINA 3622 resin processes on conventional injection molding equipment with typical melt temperatures of 390- 450°F (200-232°C)

Data provided by the manufacturer, Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 12 g/10 minASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 103ASTM D288A
Tensile Strength, Ultimate 33.1 MPaASTM D638
Elongation at Break 8.0 %ASTM D638
Modulus of Elasticity 1.38 GPaASTM D638
Flexural Modulus 1.17 GPaASTM D790
Izod Impact, Notched 0.214 J/cmASTM D256A
Izod Impact, Unnotched 9.55 J/cmASTM D256A
 
Thermal PropertiesOriginal ValueComments
Melting Point 165 °CDSC
Deflection Temperature at 0.46 MPa (66 psi) 121 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 232 °CInjection

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPH 3429 Polypropylene, Injection Molding Grade
Total PPH 3620WZ Polypropylene, Injection Molding Grade
Total PPH 3825 Polypropylene, Injection Molding Grade
Total PPR 7425 Polypropylene, Injection Molding Grade
LyondellBasell Pro-fax SR549M Polypropylene Random Copolymer, Clarified

PFIN22 / 38352

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.