MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Envalior Durethan® DP 2801 000000 Nylon 66 (PA66), Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free

Former Lanxess product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.143 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0114 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0122 cm/cm60x60x2; 280 °C / MT 80°C; 600 bar; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 2396 N
@Temperature 23.0 °C
ISO 6603-2
Ball Indentation Hardness 70.0 MPaISO 2093-1
Tensile Strength at Break 55.0 MPa5 mm/min; ISO 527-1,-2
Tensile Strength, Yield 55.0 MPa50 mm/min; ISO 527-1,-2
Elongation at Break 155 %Nominal, 50 mm/min; ISO 527-1,-2
 230 %5 mm/min; ISO 527-1,-2
Elongation at Yield 20 %50 mm/min; ISO 527-1,-2
Tensile Modulus 1400 MPa1 mm/min; ISO 527-1,-2
Flexural Strength 49.0 MPa2 mm/min; ISO 178-A
Flexural Yield Strength 36.0 MPa
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus 1300 MPa2 mm/min; ISO 178-A
Flexural Strain at Break 8.0 %2 mm/min; ISO 178-A
Izod Impact, Notched (ISO) <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180-1A
 10.0 kJ/m²
@Temperature 23.0 °C
ISO 180-1A
Izod Impact, Unnotched (ISO) 130 kJ/m²
@Temperature -30.0 °C
ISO 180-1U
 NB
@Temperature 23.0 °C
ISO 180-1U
Charpy Impact Unnotched 185 kJ/m²
@Temperature -30.0 °C
ISO 179-1eU
 NB
@Temperature 23.0 °C
ISO 179-1eU
Charpy Impact, Notched <= 10.0 kJ/m²
@Temperature -30.0 °C
ISO 179 1eA
 15.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
Puncture Energy 27.2 J
@Temperature 23.0 °C
ISO 6603-2
 
Thermal PropertiesOriginal ValueComments
Melting Point 265 °C10°C/min; ISO 11357-1,-3
 
Processing PropertiesOriginal ValueComments
Melt Temperature 260 °Cinjection molding
 260 - 270 °C
Mold Temperature 80.0 °Cinjection molding
 80.0 - 100 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 1003-2 NF2002 PA66 (Conditioned)
Plastcom SLOVAMID 66 HI/1 PA66, improved strength
Epsan Eplamid 66 IMP NC Q1C201 Polyamide 66
Envalior Durethan® DP 2325 H3.0 000000 Nylon 66 (PA66), Conditioned
Envalior Durethan® A 30 S 000000 Nylon 6 (PA6), Conditioned

PLANW9481 / 208336

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.