MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Halogenated flame retardant compound – High hardness

Uses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are required

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.29 g/ccASTM D792
Loss On Ignition 32 %ASTM D2863
Maximum Moisture Content 0.020
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 87 - 93
@Time 5.00 sec
ASTM D2240
Tensile Strength 27.9 MPaASTM D412
Elongation at Break 340 %ASTM D412/D638
100% Modulus 0.00860 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0148 GPa
@Strain 300 %
ASTM D412
Tear Strength 125 pliASTM D470
Graves Tear Strength 480 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 240H18, 1000g; ASTM D3389 B
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -38.0 °CDSC
Flammability Test 5.0
 
Processing PropertiesOriginal ValueComments
Zone 1 183 °CExtrusion
Zone 2 188 °CExtrusion
Zone 3 196 °CExtrusion
Zone 4 199 °CExtrusion
Adapter Temperature 202 °C5, Extrusion
Die Temperature 196 °CZone 2, Extrusion
 202 °CZone 1, 6, Extrusion
Drying Temperature 104 °C
Dry Time 2.00 - 4.00 hour
Dew Point -40.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58212 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58202 Ether Based Thermoplastic Polyurethane
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane
Lubrizol Estane® 58070 Thermoplastic Polyurethane
Lubrizol ESTANE® 58213 Ester Based Thermoplastic Polyurethane

PNOVEON032 / 55298

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.