MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
HP Alloys Nitronic® 50 Austenitic Stainless, Annealed
Categories: Metal; Ferrous Metal; Heat Resisting; Stainless Steel; T S20000 Series Stainless Steel

Material Notes: Annealed applies to tensile, impact, and hardness values and are for 3/4 in. diameter samples; other properties are typical of this alloy.

Nitronic® 50 Stainless Steel provides a combination of corrosion resistance and strength not found in any other commercial material available in its price range. This austenitic stainless has corrosion resistance greater than that provided by Types 316 and 316L, plus approximately twice the yield strength at room temperature. In addition, Armco Nitronic 50 Stainless has very good mechanical properties at both elevated and sub-zero temperatures. And, unlike many austenitic stainless steels, Nitronic 50 does not become magnetic when cold worked.

Data provided by High Performance Alloys, Inc.

Key Words: Bar ASTM A276 ASTM A479, AMS 5764; Plate/Sheet ASTM A240, ASTM A412, AMS 5861, Pipe & Tube SPECIALS, ASTM A312, ASTM A403, UNS S20910; Forgings ASTM A314; Fasteners ASTM A193/ASTMA194; Welding Wire AWS ER209; NACE MR-01-75
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.88 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 189Estimated from Rockwell B
Hardness, Knoop 232Estimated from Rockwell B
Hardness, Rockwell A 56Estimated from Rockwell B
Hardness, Rockwell B 91
Hardness, Vickers 193Estimated from Rockwell B
Tensile Strength, Ultimate 800 MPa
Tensile Strength, Yield 393 MPa
@Strain 0.2 %
Elongation at Break 47 %
Reduction of Area 70 %
Tensile Modulus 193 GPa
Charpy Impact 314 J
@Temperature 27.0 °C
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000110 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 95.0 °C
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr 22 %
Iron, Fe 58 %As remainder
Manganese, Mn 5.0 %
Molybdenum, Mo 2.25 %
Nickel, Ni 12.5 %
Nitrogen, N 0.30 %
Silicon, Si <= 1.0 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MetalTek MTEK 6 UNS R30006 Cobalt Base Alloy
Carlson Nitronic® 50® Austenitic Stainless Steel
HP Alloys Nitronic® 50 Austenitic Stainless, Level 1 Cold Worked
AISI Type S20910 Stainless Steel, high strength
MetalTek Nitronic® 50 Cast UNS J93790 Austenitic Stainless Steel

NN5000 / 18443

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.