MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Skamol Group V-LITE 375 Vermiculite Insulating Brick  (discontinued **)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: V-LITE vermiculite insulating bricks have the following characteristics:
  • Max. service temperature 1100°C (2012°F)
  • Hot-face applications and back-up insulation
  • Good insulation value
  • High mechanical strength
  • High temperature resistance, withstand direct flame impingement
  • Can be used in furnaces with reducing atmospheres due to their resistance to carbon monoxide and hydrocarbon attacks
  • Equally suitable for hot-face applications and back-up insulation of refractory constructions
  • Used for lining in all types of industrial kilns and furnaces, incinerators and combustion plants

Information provided by Skamol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 23.4 lb/ft³Dry
Loss On Ignition 7.0 %
@Temperature 1025 °C
Porosity 86 %Total
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.000500 GPaEN 993-6: 1995
Compressive Strength 1.30 MPaEN 1094-5: 1995
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.0 µm/m-°C
@Temperature 20.0 - 750 °C
BS 1902: section 5.3: 1990
Specific Heat Capacity 0.940 J/g-°C
Thermal Conductivity 0.120 W/m-K
@Temperature 200 °C
Mean temp.; ASTM C-182
 0.140 W/m-K
@Temperature 400 °C
ASTM C-182
 0.160 W/m-K
@Temperature 600 °C
ASTM C-182
Maximum Service Temperature, Air 1100 °C
Shrinkage 1.0 %
@Temperature 1000 °C,
Time 43200 sec
Linear Reheat Shrinkage; EN 1094-6: 1999
 
Component Elements PropertiesOriginal ValueComments
Al2O3 7.0 %
CaO 2.0 %
Fe2O3 4.0 %
K2O 11 %
MgO 21 %
Na2O 0.50 %
SiO2 47 %
TiO2 0.50 %
 
Descriptive Properties
ColorLight Brown
Pyrometric Cone Equivalent1300°CASTM C24-89, ORTON cones
Resistance to Thermal ShockMin 10 cyclesEN 993-11: 1998, heating to 950°C (1742°F)

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Concrete, expanded clay aggregate
BNZ Materials 375 Insulating Cement
Concrete, gravel or crushed stone aggregate
Concrete, expanded perlite aggregate
Avient Edgetek® PP-15GF/000 Polypropylene (PP), Glass Filled

CSKAM011 / 2162

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.