MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kingfa MAC-601 UV PC/ABS Alloy
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes:
    Features:
  • Excellent balance properties
  • High impact strength
  • Good processing properties

    Applications:
  • Injection molding
  • Automobile instrument panel
  • Electrical and electronic parts
  • Computer and accessories
  • Household appliance thin wall parts

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.13 g/cc
@Temperature 23.0 °C
ASTM D792
Water Absorption 0.30 %
@Temperature 23.0 °C,
Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm
@Temperature 23.0 °C
ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 50.0 MPa50mm/min; ASTM D638
Elongation at Break 60 %50mm/min; ASTM D638
Flexural Strength 75.0 MPa2mm/min; ASTM D790
Flexural Modulus 2100 MPa2mm/min; ASTM D790
Izod Impact, Notched 500 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
Izod Impact, Unnotched NB
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+12 ohm-cmASTM D257
Surface Resistance 1.00e+13 ohmASTM D257
Dielectric Strength >= 35.0 kV/mm1.6mm; ASTM D149
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 125 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
@Thickness 6.40 mm
ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
 HB
@Thickness 3.20 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 280 °C
Rear Barrel Temperature 230 - 250 °CStart Point: 230°C
Middle Barrel Temperature 240 - 260 °CStart Point: 235°C
Front Barrel Temperature 250 - 280 °CStart Point: 240°C
Melt Temperature 240 - 280 °CStart Point: 245°C
Mold Temperature 60.0 - 90.0 °CStart Point: 60°C
Drying Temperature 100 - 110 °C
@Time 14400 - 21600 sec
Pre-dry
Back Pressure 0.700 - 1.00 MPa
 
Descriptive Properties
Injection Speed60-100%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa MAC-601 AC PC/ABS Alloy
Kingfa MAC-301 PC/ABS Alloy
Kingfa MAC-501 Modified PC/ABS Alloy
Kingfa MAC-601 DY Modified 60/40 PC/ABS Alloy
Kingfa MAC-451PG Electroplating PC/ABS Alloy

PKINGF064 / 104323

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.