MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mid-Mountain Materials CERMEX® MT1000 Needled Fiberglass Mat
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: CERMEX® MT1000 fiberglass mat is comprised of high purity, highly resilient E-Glass fibers. CERMEX® MT1000 is lightweight, strong, and highly efficient as insulation in most high heat environments for extended periods at elevated temperatures. The absence of organic or synthetic binders makes this product smoke-free on heat-up and allows the product to remain mechanically stable even after exposure to extreme temperatures. Needled and Felted Blanket.

Information provided by Mid-Mountain Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.00 - 11.0 lb/ft³
Thickness 6350 microns
 12700 microns
 25400 microns
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0576 W/m-K
@Temperature 149 °C
 0.0721 W/m-K
@Temperature 260 °C
 0.0937 W/m-K
@Temperature 371 °C
Melting Point 1120 °C
Maximum Service Temperature, Air 1000 °FContinuous
 1500 °FShort term
 
Descriptive Properties
Roll Length (ft)1501/4"
 451"
 751/2"
Sound Absorption Coefficient (Sabin/ft2)0.04 ±0.041/4" thick, 250 Hz
 0.07 ±0.021/2" thick, 250 Hz
 0.17 ±0.021/4" thick, 500 Hz
 0.29 ±0.041" thick, 250 Hz
 0.30 ±0.031/2" thick, 500 Hz
 0.30 ±0.031/4" thick, 1000 Hz
 0.68 ±0.031/4" thick, 2000 Hz
 0.72 ±0.081/2" thick, 1000 Hz
 0.86 ±0.031" thick, 500 Hz
 0.92 ±0.031" thick, 2000 Hz
 0.94 ±0.051/2" thick, 2000 Hz
 0.94 ±0.051/4" thick, 4000 Hz
 0.95 ±0.041" thick, 1000 Hz
 0.95 ±0.051" thick, 4000 Hz
 0.97 ±0.051/2" thick, 4000 Hz
Width (in)60

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Fiberglass Grade B
Mid-Mountain Materials PADMAT® MT1000 Needled Fiberglass Mat
Mid-Mountain Materials HYTEX® 1000 Fiberglass Industrial Textile
AGY ADVANTEX® Generic Glass Fiber
Mid-Mountain Materials HYTEX® 1400 Fiberglass Industrial Textile

CMID63 / 141231

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.