MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Solvay SUPRAGIL® MNS-88 Condensed methyl naphthalene sulfonate, sodium salt
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Condensed methyl naphthalene sulfonate, sodium salt. Dispersing agent for wettable powders, concentrated suspensions and water dispersible granules , binding properties. Particularly suitable for high concentration water dispersible granules.

Identification: SULFONATED AROMATIC CONDENSATE, SODIUM SALT

CAS: 68425-94-5

Available in: Asia Pacific, Europe, Latin America and North America

Applications: SUPRAGIL MNS-88 is a condensed methyl naphthalene sulfonate, sodium salt. Dispersing agent for wettable powders, concentrated suspensions and water dispersible granules, binding properties. Particularly suitable for high concentration water dispersible granules.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 7.5 - 105% Solution; RP-0420
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 4.0 %RP-17505
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceTan powder
CompositionActive>88%, RP-18119
 Free Oil<2.5%, RP-17608
 Sodium Sulfate7-9%, RP-17503

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay SUPRAGIL® MNS/90 Condensed methyl naphthalene sulfonate, sodium salt
Solvay GERONOL® TE 300 Surfactant
Solvay SUPRAGIL® WP Sodium Isopropyl Naphthalene Sulfonate
Solvay SUPRAGIL® GN 4-4’ Dihydroxydiphenyl Sulphonate Condensate Sodium Salt
Solvay GERONOL® MS Surfactant

WRHOD540 / 137771

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.