MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kumho Polychem 1730N/B Thermoplastic Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Technical Feature: Low Specific Gravity; Excellent Chemical Resistance & heat Resistance; Excellent Electrical Insulation; Low Permanent Set & Compression Set; Excellent Flex Fatigue Resistance; Excellent Tear Strength; Excellent Ozone-Resistance & Weather Resistance; Recycling
It is manufactured and supplied in pellet form for easy handling and storage; It may absorb a significant amount of moisture from the atmosphere. INNOPRENE, when exposed to humidity, develops an uneven surface and degraded physical properties. Therefore, be user to dry INNOPRENE for 2-3 hrs and 80-90°C, before processing.

Applications
Automotive: Tubing, Gaskets, Door seals, Dust covers, Impact plates, Interiors, Tubes, Front glass seals, Door belt, Glassrun channel, Bellows, Air intake hose, Wiper & Spoiler, Bumper mud guard, Inpanel skin, Airbag cover/blanket & Holder, Etc.
Construction: Glass seals, Expansion joints, Light bulb gaskets, Window seals, Waterproof roofing sheet, Flooring sheet, Track sheet, Etc.
Office Equipment: Anti-vibration, Feed rollers, Guards, Anti slipping pad, Etc.
Appliances: Hose connectors, Doors seals, Interior/Exterior materials, Hoses, Gaskets, Motor mounts, Lever peaks, Electric cleaner wheels, Insulator seals, Light insulator rings, Etc.
Electrical Equipment: Syringe tips, Medical devices wheels, Power transmitters/receivers, Connectors, Mine cables, Control cables, Coil cords, Power circuit cables, Etc.
Sports Equipment: Underwater devices for divers, Fishing pole grips, Ski pole grips, Outdoor stuff. Etc.

Information provided by Kumho Polychem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.950 g/cc0.950 g/ccASTM D297
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8989ISO 868
 91
@Temperature 150 °C,
Time 605000 sec
91
@Temperature 302 °F,
Time 168 hour
Heat Aging; ISO 888
Tensile Strength 14.7 MPa2130 psiASTM D412
 12.21 MPa
@Temperature 150 °C,
Time 605000 sec
1771 psi
@Temperature 302 °F,
Time 168 hour
Heat Aging; ASTM D412
Elongation at Break 570 %570 %ASTM D412
 473.1 %
@Temperature 150 °C,
Time 605000 sec
473.1 %
@Temperature 302 °F,
Time 168 hour
Heat Aging; ASTM D412
100% Modulus 5.88 MPa853 psiASTM D412
Tear Strength 78.5 kN/m448 pliASTM D624
Compression Set  55 %
@Temperature 70.0 °C,
Time 79200 sec
55 %
@Temperature 158 °F,
Time 22.0 hour
ASTM D395-03
 70 %
@Temperature 120 °C,
Time 252000 sec
70 %
@Temperature 248 °F,
Time 70.0 hour
ASTM D395-03
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -61.0 °C-77.8 °FISO 812, Type B
 
Descriptive Properties
Fluid resistance (% weight change)+210% HCl, 25°C x 168hr
 050% NaOH, 25°C x 168hr
UV resistance<21000 hr, SAE J1960

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKUMHO036 / 313391

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.