MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6/66; Nylon 66/6, 60% Glass Fiber Reinforced

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.58 - 1.72 g/cc0.0571 - 0.0621 lb/in³Average value: 1.68 g/cc Grade Count:27
Filler Content 60.0 %60.0 %Average value: 60.0 % Grade Count:6
Water Absorption 0.350 - 5.00 %0.350 - 5.00 %Average value: 2.07 % Grade Count:16
Moisture Absorption at Equilibrium 1.10 - 1.40 %1.10 - 1.40 %Average value: 1.23 % Grade Count:9
 1.10 - 1.10 %
@Temperature 70.0 - 70.0 °C
1.10 - 1.10 %
@Temperature 158 - 158 °F
Average value: 1.10 % Grade Count:4
Water Absorption at Saturation 3.50 - 4.00 %3.50 - 4.00 %Average value: 3.80 % Grade Count:12
Linear Mold Shrinkage 0.00100 - 0.00600 cm/cm0.00100 - 0.00600 in/inAverage value: 0.00250 cm/cm Grade Count:18
 0.00100 - 0.00100 cm/cm
@Temperature 80.0 - 80.0 °C
0.00100 - 0.00100 in/in
@Temperature 176 - 176 °F
Average value: 0.00100 cm/cm Grade Count:4
Linear Mold Shrinkage, Transverse 0.00100 - 0.00900 cm/cm0.00100 - 0.00900 in/inAverage value: 0.00425 cm/cm Grade Count:15
 0.00300 - 0.00300 cm/cm
@Temperature 80.0 - 80.0 °C
0.00300 - 0.00300 in/in
@Temperature 176 - 176 °F
Average value: 0.00300 cm/cm Grade Count:4
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 198 - 350 MPa28700 - 50800 psiAverage value: 281 MPa Grade Count:12
Tensile Strength, Ultimate 155 - 280 MPa22500 - 40600 psiAverage value: 228 MPa Grade Count:26
 150 - 160 MPa
@Temperature 80.0 - 80.0 °C
21800 - 23200 psi
@Temperature 176 - 176 °F
Average value: 155 MPa Grade Count:2
Tensile Strength, Yield 135 - 270 MPa19600 - 39200 psiAverage value: 192 MPa Grade Count:3
Elongation at Break 2.00 - 4.00 %2.00 - 4.00 %Average value: 2.43 % Grade Count:29
 2.30 - 2.80 %
@Temperature 80.0 - 80.0 °C
2.30 - 2.80 %
@Temperature 176 - 176 °F
Average value: 2.55 % Grade Count:2
Modulus of Elasticity 13.0 - 22.5 GPa1890 - 3260 ksiAverage value: 18.4 GPa Grade Count:24
 10.0 - 13.0 GPa
@Temperature 80.0 - 80.0 °C
1450 - 1890 ksi
@Temperature 176 - 176 °F
Average value: 11.5 GPa Grade Count:2
Flexural Yield Strength 290 - 450 MPa42100 - 65300 psiAverage value: 379 MPa Grade Count:10
 290 - 290 MPa
@Temperature 80.0 - 80.0 °C
42100 - 42100 psi
@Temperature 176 - 176 °F
Average value: 290 MPa Grade Count:2
Flexural Modulus 1.76 - 22.5 GPa255 - 3260 ksiAverage value: 16.4 GPa Grade Count:10
 13.0 - 13.0 GPa
@Temperature 80.0 - 80.0 °C
1890 - 1890 ksi
@Temperature 176 - 176 °F
Average value: 13.0 GPa Grade Count:2
Izod Impact, Notched 1.60 - 1.87 J/cm3.00 - 3.50 ft-lb/inAverage value: 1.73 J/cm Grade Count:4
Izod Impact, Unnotched (ISO) 76.0 - 80.0 kJ/m²
@Temperature -30.0 - -30.0 °C
36.2 - 38.1 ft-lb/in²
@Temperature -22.0 - -22.0 °F
Average value: 78.0 kJ/m² Grade Count:2
Charpy Impact Unnotched 5.50 - 11.5 J/cm²26.2 - 55.0 ft-lb/in²Average value: 9.72 J/cm² Grade Count:24
 5.50 - 10.5 J/cm²
@Temperature -30.0 - -20.0 °C
26.2 - 50.0 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 8.74 J/cm² Grade Count:20
Charpy Impact, Notched 1.10 - 5.00 J/cm²5.24 - 23.8 ft-lb/in²Average value: 2.96 J/cm² Grade Count:24
 1.00 - 4.50 J/cm²
@Temperature -30.0 - -20.0 °C
4.76 - 21.4 ft-lb/in²
@Temperature -22.0 - -4.00 °F
Average value: 2.95 J/cm² Grade Count:20
Puncture Energy 31.0 - 31.0 J
@Temperature -30.0 - -30.0 °C
22.9 - 22.9 ft-lb
@Temperature -22.0 - -22.0 °F
Average value: 31.0 J Grade Count:1
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+10 - 1.00e+15 ohm-cm1.00e+10 - 1.00e+15 ohm-cmAverage value: 5.46e+13 ohm-cm Grade Count:16
Surface Resistance 1.00e+10 - 8.00e+13 ohm1.00e+10 - 8.00e+13 ohmAverage value: 1.03e+13 ohm Grade Count:11
Dielectric Strength 18.9 - 40.0 kV/mm480 - 1020 kV/inAverage value: 26.2 kV/mm Grade Count:13
Comparative Tracking Index 55.0 - 600 V55.0 - 600 VAverage value: 526 V Grade Count:10
 
Thermal PropertiesMetricEnglishComments
CTE, linear 12.6 - 20.0 µm/m-°C7.00 - 11.1 µin/in-°FAverage value: 18.3 µm/m-°C Grade Count:9
CTE, linear, Transverse to Flow 39.6 - 87.0 µm/m-°C22.0 - 48.3 µin/in-°FAverage value: 47.0 µm/m-°C Grade Count:8
Melting Point 238 - 265 °C460 - 509 °FAverage value: 256 °C Grade Count:21
Maximum Service Temperature, Air 100 - 230 °C212 - 446 °FAverage value: 173 °C Grade Count:9
Deflection Temperature at 0.46 MPa (66 psi) 255 - 257 °C491 - 495 °FAverage value: 256 °C Grade Count:3
Deflection Temperature at 1.8 MPa (264 psi) 225 - 255 °C437 - 491 °FAverage value: 242 °C Grade Count:18
Deflection Temperature at 8.0 MPa 195 - 235 °C383 - 455 °FAverage value: 223 °C Grade Count:13
Flammability, UL94 HB - 5VAHB - 5VAGrade Count:17
 
Processing PropertiesMetricEnglishComments
Melt Temperature 225 - 320 °C437 - 608 °FAverage value: 289 °C Grade Count:8
Mold Temperature 65.0 - 120 °C149 - 248 °FAverage value: 93.3 °C Grade Count:6
Drying Temperature 70.0 - 90.0 °C158 - 194 °FAverage value: 79.9 °C Grade Count:7
Moisture Content 0.0500 - 0.200 %0.0500 - 0.200 %Average value: 0.147 % Grade Count:7
Injection Pressure 34.5 - 150 MPa5000 - 21800 psiAverage value: 119 MPa Grade Count:4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66/6
Overview of materials for Nylon 6, 50% Glass Fiber Filled
Overview of materials for Nylon 66/6, 20% Glass Fiber Reinforced
Overview of materials for Nylon 66/6, 40% Glass Fiber Reinforced
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced

O2496 / 77997

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.