MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC LNP™ LUBRICOMP™ Compound KFL23LH Acetal (POM) Copolymer (Americas)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: LNP LUBRICOMP KFL23LH compound is based on Acetal (POM) Copolymer resin containing 15% glass fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Low Extractable.

Features: Low Extractable,Healthcare,Wear resistant,Food Contact Acceptable

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.58 g/ccASTM D792
Density 1.58 g/ccASTM D792
Moisture Absorption 0.210 %23°C/50% RH/24 hrs; ASTM D570
 0.340 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0090 - 0.020 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.010 - 0.030 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 75.0 MPa5 mm/min; ISO 527
 78.0 MPa5 mm/min; ASTM D638
Elongation at Break 1.7 %5 mm/min; ISO 527
 1.8 %5 mm/min; ASTM D638
Tensile Modulus 6720 MPa50 mm/min; ASTM D638
 6820 MPa1 mm/min; ISO 527
Flexural Strength 107 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
 108 MPaISO 178
 119 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 5740 MPa1.3 mm/min, 50 mm span; ASTM D790
 5900 MPa2 mm/min; ISO 178
Izod Impact Notched 50.0 JASTM D256
Izod Impact, Unnotched 500 J/mASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 22.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 10.0 JASTM D3763
Impact Test 2.00 JMultiaxial Impact; ISO 6603
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 163 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 163 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 158 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 161 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Zone 2 195 - 205 °C
Zone 3 210 - 220 °C
Melt Temperature 200 - 215 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 80.0 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80826 / 288773

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.