MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT Group EP AJS EPI Engineered Polymers Aliphatic Joint Sealant
Categories: Polymer; Thermoset

Material Notes: EP AJS Aliphatic Joint Sealant, “Powered by Reactamine® Technology, is a two component 100% solid, aliphatic (silicone optional) polyurea based joint sealant. EP AJS is a self-leveling joint sealant designed to protect interior horizontal concrete expansion and control joints from spalling, chipping, and breakdown. This elastomer displays fast cure times and excellent adhesion to concrete. EP AJS can be applied at temperatures ranging -30° F to 250°F. This polyurea elastomer displays excellent chemical resistance, water insensitivity, and thermal stability at high and low temperatures. EP AJS may also be used under traditional floor coatings (such as epoxies, polyureas and polyurethanes) or tiles to smooth the joints and provide protection from cracking and sinking caused by non-elastomeric joint sealants. EP AJS has outstanding color stability.

ApplicationsEP AJS was designed to protect against the abuse to concrete joints caused by heavy load transfers from such items as forklifts, steel-wheeled carts and trash dumpsters. Some typical uses include:

  • Concrete Control / Expansion Joints
  • Concrete Spall Repairs
  • Cold Storage Facilities
  • Merchandise Distribution Centers
  • Home Improvement Stores
  • Bridge Headers
  • Warehouse Floors
  • D.O.T. Pothole Road Repair
  • U.S.D.A. and F.D.A. Acceptable
  • Part of the Amber Chemical Group. Data provided by manufacturer.

    Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesOriginal ValueComments
    Viscosity 350 cPB Side
     650 cPA Side
     
    Mechanical PropertiesOriginal ValueComments
    Hardness, Shore A 85ASTM D2240
    Tensile Strength 1250 psiASTM D412
    Elongation at Break 450 %ASTM D412
    100% Modulus 1.10 ksi
    @Strain 100 %
    ASTM D412
    Tear Strength 350 pliASTM D412
    Taber Abrasion, mg/1000 Cycles 20.5CS17 Wheel, 1kg; ASTM D4060
     
    Processing PropertiesOriginal ValueComments
    Tack-Free Time >= 0.167 hour
    Gel Time 2.00 min
     
    Descriptive Properties
    Flexibility PassASTM D1737, 1/8"Mandrel

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    Users viewing this material also viewed the following:
    Evonik TEGO® Antifoam 5-27 Emulsion
    Concrete, Highstrength
    CHT Group ReactAmine® EP 350 EPI Engineered Polymers Polyurea
    CHT Group EP JS EPI Engineered Polymers Joint Sealant
    BASF Styrodur® 5000 CS Extruded Rigid Polystyrene Foam (Europe)

    PACC103 / 22230

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.