MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LATI Latistat 52/7-02 MI/30 PP Homopolymer, 30% Mica Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 30% Mica Filler

Material Notes: Dissipative product based on Polypropylene homopolymer (PPh). Mica filler.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Information provided by Lati Industria Termoplastici S.p.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/cc
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm
Linear Mold Shrinkage, Transverse 0.0085 - 0.0105 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 30.0 MPa
Elongation at Break 3.0 %
Elongation at Yield 1.5 %
Tensile Modulus 5200 MPa
Charpy Impact Unnotched 10.0 kJ/m²
Charpy Impact, Notched 1.00 kJ/m²
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 800 ohm
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
Vicat Softening Point 110 °C
@Load 5.00 kg
 
Processing PropertiesOriginal ValueComments
Melt Temperature 200 - 240 °C
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 80.0 - 90.0 °C
@Time 10800 sec
 
Descriptive Properties
ISO Shrinkage - Pressure60 MPa

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aclo Accutech Polypropylene Copolymer CP0436M30L Mica Reinforced
Aclo Accutech Polypropylene Copolymer CP0437M30L Mica Reinforced
Lushan PP+GF30% Maleic Anhydride Grafted Polypropylene
Crystex Composites Mykroy/Mycalex MM 561 Molding Grade Glass-bonded Mica Composite
Adell RQ-16 Copolymer Polypropylene, 30% Mica Reinforced

PLATH9980 / 177676

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.