MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem H 201 Injection Molding Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Description: H 201 is a high melt flow rate additivated homopolymer suitable for injection molding and fiber extrusion applications. This product exhibits excellent processability with good melt stability and stiffness/impact strength balance. It also features low taste/odor transfer.

Applications: Injection of electric portables and household appliances; Injected chest of drawers and closets; Continuous filaments for carpets, sewing threads and ropes; Staple fibers for rugs and blankets; Nonwovens produced by thermobonded process.

Information provided by Braskem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D792A
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238L
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Tensile Strength, Yield 35.0 MPaASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus, 1% Secant 1.50 GPaASTM D790
Izod Impact, Notched 20.0 J/m
@Temperature 23.0 °C
ASTM D256A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 107 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 57.0 °CASTM D648
Vicat Softening Point 154 °C10 N; ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman ComAlloy Aqualoy® 125 Polypropylene, Glass Reinforced, Chemically Coupled NSF, UL
Braskem H 306 Injection Molding Polypropylene
Braskem Prisma 3410 RACO Random Polypropylene Copolymer
Formosa Plastics Formolene® 2315A Injection Molding Polypropylene
Braskem HC7260LS-L HDPE Injection Molding Polyethylene

PBRAS022 / 27756

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.