MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese 520 Film LDPE polymer for flexible packaging
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: 520 is recommended for general film resin. Properties listed are for a film produced on a 20:1 L/D, 65 mm extruder with a 130 mm die, at a stock temperature of 205°C. Additives:

Applications: Flexible Packaging

Information provided by Celanese Corporation.

Key Words: general film resin
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.921 g/ccAT Plastics PTM-03
Thickness 50.0 microns
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 12.0 MPaMethod A (500 mm/min); ASTM D882
Film Tensile Strength at Yield, TD 12.0 MPaMethod A (500 mm/min); ASTM D882
Film Elongation at Break, MD 400 %Method A (500 mm/min); ASTM D882
Film Elongation at Break, TD 600 %Method A (500 mm/min); ASTM D882
Secant Modulus, MD 0.210 GPa1% Secant Modulus; ASTM D882
Secant Modulus, TD 0.240 GPa1% Secant Modulus; ASTM D882
Dart Drop 2.00 g/micronf50; ASTM D1709
Film Tensile Strength at Break, MD 21.0 MPaMethod A (500 mm/min); ASTM D882
Film Tensile Strength at Break, TD 20.0 MPaMethod A (500 mm/min); ASTM D882
 
Optical PropertiesOriginal ValueComments
Haze 14 %ASTM D1003
Gloss 54 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Processing Temperature 170 - 230 °C
Blow-up Ratio (BUR) 2.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Amco PRIMATOP LDPE 023919 Blow Molding Polyethylene
Albis Plastics Tedur® L V 9400-1 PPS, 15% Carbon Fiber
Albis Plastics Tedur® L V 9300-1 PPS, 40% Glass Fiber/Glass Bead
Albis Plastics Tedur® L V 9107-1 PPS, 40% Glass Fiber
Afton Plastics 450HP PFA Welding Rod

PATEVB60 / 26016

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.