System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Entec Hylex® P1302B Polycarbonate
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
;
Polycarbonate, Molded
Material Notes:
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.
Information provided by Entec.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Water Absorption
0.15 %
0.15 %
24 hrs; ASTM D570
Melt Flow
2.3
g/10 min
@Load 1.20 kg,
Temperature 300 °C
2.3
g/10 min
@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell M
122
122
ASTM D785
Tensile Strength at Break
68.9
MPa
10000
psi
ASTM D638
Elongation at Break
100 %
100 %
ASTM D638
Flexural Strength
88.3
MPa
12800
psi
ASTM D790
Flexural Modulus
2.07
GPa
300
ksi
ASTM D790
Izod Impact, Notched
8.33
J/cm
15.6
ft-lb/in
73°F, 0.125 in; ASTM D256
Thermal Properties
Metric
English
Comments
Deflection Temperature at 0.46 MPa (66 psi)
138
°C
280
°F
Unannealed (0.125 in); ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)
132
°C
270
°F
Unannealed (0.125 in); ASTM D648
Glass Transition Temp, Tg
152
°C
306
°F
Transition Temperature, tested in accordance with ASTM D1525; ASTM E1356
Optical Properties
Metric
English
Comments
Refractive Index
1.585
1.585
ASTM D542
Transmission, Visible
78 %
78 %
125 mil; ASTM D1003
Processing Properties
Metric
English
Comments
Zone 1
229
-
249
°C
445
-
480
°F
Zone 2
241
-
260
°C
465
-
500
°F
Zone 3
249
-
271
°C
480
-
520
°F
Zone 4
249
-
271
°C
480
-
520
°F
Adapter Temperature
246
-
266
°C
475
-
510
°F
Die Temperature
254
-
277
°C
490
-
530
°F
Head Temperature
249
-
271
°C
480
-
520
°F
Zone 2
254
-
277
°C
490
-
530
°F
Zone 1
Mold Temperature
110
-
129
°C
230
-
265
°F
Drying Temperature
121
°C
250
°F
Dry Time
3
-
4
hour
3
-
4
hour
Moisture Content
<= 0.020 %
<= 0.020 %
Screw Speed
20
-
40
rpm
20
-
40
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Covestro Makrolon® ET3227 Polycarbonate
Covestro Makrolon® 8345 Polycarbonate
Covestro Makrolon® 3207 Polycarbonate
Entec Hylex® P1007L1 HB Polycarbonate
Entec Hylex® P1017L2 HB Polycarbonate
PENT052 / 36080
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.