MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Corning Gorilla® Glass SR+ Touch Screen Glass  (discontinued **)
Categories: Ceramic; Glass; Optical

Material Notes: Gorilla® Glass SR+ is a glass composite designed for wearables such as watches that combines the toughness, optical clarity and touch sensitivity of Gorilla Glass with superior scratch resistance approaching that of luxury watch cover materials. Resists common environmental exposures such as sunscreen, salt water, temperature, etc.

Information provided by Corning Incorporated.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 400 - 2000 microns15.7 - 78.7 mil
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %
@Wavelength 400 - 760 nm
90 %
@Wavelength 400 - 760 nm
Reflection Coefficient, Visible (0-1) 0.10
@Wavelength 400 - 760 nm
0.10
@Wavelength 400 - 760 nm
First Surface Reflectance
 
Descriptive Properties
Color a-1.51 to 0.27
Color b-3.16 to 0.79

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 6061-O
Carpenter Super Invar 32-5
Borosilicate Glass
Corning Gorilla® Glass 3 Touch Screen Glass with NDR
Corning Gorilla® Glass 5 Display Glass

CCORNG14j / 197401

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.