MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Wacker® Silane IO-TRIMETHOXY
Categories: Fluid

Material Notes: Empirical formula: C11H26O3Si

CAS No.: 34396-03-7

SILANE IO-TRIMETHOXY is a clear, colorless liquid with a characteristic odor.

The use of SILANE IO-TRIMETHOXY to render fillers water repellent considerably improves their dispersibility and reduces their sedimentation tendency. Mineral-filled plastics can thus be processed more easily. SILANE IO-TRIMETHOXY is suitable for waterrepellent impregnation of construction materials (especially concrete and reinforced concrete). It increases their resistance to alkalis and reduces water absorption, thus improving durability. As an ingredient in silane-crosslinking formulations, SILANE IO-TRIMETHOXY can be used to influence mechanical properties and curing behavior.

Special features: SILANE IO-TRIMETHOXY is a mixture of isomeric octyltrimethoxysilanes, with iso-octyltrimethoxysilane as the main component. SILANE IO-TRIMETHOXY is practically insoluble in water. The silanes hydrolyze slowly in the presence of moisture (methanol is released) to form reactive silanols, which can then react with themselves to produce siloxanes.

SILANE IO-TRIMETHOXY is used to render a wide range of surfaces and materials water repellent (e.g. construction materials, fillers). SILANE IOTRIMETHOXY is also used in the production of silanecrosslinking formulations.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccDIN 51757
Viscosity 1.6 cPdynamic; DIN 51562
Molecular Weight 234.4 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 90.0 °C
@Pressure 0.1013 MPa
Flash Point >= 52.0 °CISO 2719

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Wacker Silres® BS 38 Silicone Masonry Water Repellent
Tetrafluorosilane, SiF4
Teknor Apex APEX® 3801-60NT1 Polyvinyl Chloride, Flexible
RTP Company RTP 3801 Polyaryletherketone (PAEK), Glass Fiber 10%
NuSil MED-1055 Silicone, One Part Adhesive/Sealant - Restricted Medical Use

PWACK9809 / 205338

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.