MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Rogers Arlon Thermabond® R37340X008 Primerless Electronic Adhesive  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone; Silicone Rubber

Material Notes: Liner: 1 mil FEP; Product: uncured Silicone Rubber; Carrier: 3 mil PTFE coated fiberglas

Information provided by Arlon Silicone Technologies; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.85 g/cc1.85 g/ccArlon SQA-TMS-024
Thickness 203 microns8.00 milArlon SQA-TMS-003
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8787ASTM D2240
Tensile Strength, Ultimate 2.52 MPa365 psiASTM D412
Elongation at Break 28 %28 %ASTM D412
Modulus of Elasticity 0.0621 GPa9.00 ksiArlon SQA-TMS-008
Poissons Ratio 0.500.50
Shear Modulus 0.00183 GPa0.265 ksiASTM D1002
Shear Strength 0.965 MPa140 psiASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 4.6024.602IPC TM 650-2.5.5.3
Dielectric Strength 35.4 kV/mm900 kV/inASTM D149
Dissipation Factor 0.00410.0041IPC TM 650-2.5.5.3
 
Thermal PropertiesMetricEnglishComments
CTE, linear 52.0 µm/m-°C
@Temperature 20.0 °C
28.9 µin/in-°F
@Temperature 68.0 °F
ASTM E 831
Specific Heat Capacity 0.850 J/g-°C
@Temperature 100 °C
0.203 BTU/lb-°F
@Temperature 212 °F
Arlon SQA-TMS-052
Thermal Conductivity 3.00 W/m-K20.8 BTU-in/hr-ft²-°FSilicone property; ASTM E1530
 3.3867 W/m-K
@Temperature 100 °C
23.504 BTU-in/hr-ft²-°F
@Temperature 212 °F
SQA-TMS-054
Maximum Service Temperature, Air 95.6 °C204 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
Glass Transition Temp, Tg -119 °C-182 °FASTM D3418
 
Processing PropertiesMetricEnglishComments
Cure Time 15.0 min
@Temperature 121 °C
0.250 hour
@Temperature 250 °F
Shelf Life 6.00 Month
@Temperature 7.00 °C
6.00 Month
@Temperature 44.6 °F
 
Descriptive Properties
ColorGray
Plasticity (mm) Arlon SQA-TMS-0057.1

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Arlon 56976XA026 Silicone Rubber/Fiberglass Laminate
SAE 950A HSLA Steel
SAE 950X HSLA Steel
Rogers Arlon 10502R030 0.040" (1.02 mm) Cured/Post-Cured Unsupported Silicone Rubber
Rogers Arlon 10502R020 0.020" (0.508 mm) Cured Silicone Rubber (Unsupported)

PARL057 / 79709

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.