MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CRG Industries Advantic™ 30 Syntactic Foam
Categories: Polymer; Thermoset

Material Notes: Advantic is a series of lightweight, engineered foams consisting of manufactured glass, polymer, or ceramic hollow spheres embedded in a resin matrix, such as epoxy or cyanate ester. CRG Industries’ proprietary mixing process produces foams with low densities, high uniformity, and minimum voids. Advantic also exhibits high compressive strength. Typical applications include underwater buoyancy, structural core for aerospace components, dielectric applications, blast mitigation, and sporting equipment. Advantic can be easily machined using standard carbide-tipped tools.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.500 g/cchelium pycnometer
Water Absorption <= 2.0 %after 213 days; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 4250 psiASTM D695
Compressive Modulus 1.10 GPaASTM D695
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0840 W/m-KASTM D5930
Maximum Service Temperature, Air 90.0 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Hexcel® HexPly® 954-3 Curing Cyanate Resin
Park Aerospace Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced
CRG Industries Advantic™ 40 Syntactic Foam
Hexcel® HexPly® 954-3A Curing Cyanate Resin
Park Aerospace Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg

PCRG960 / 93489

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.