MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Washington Penn PPH5CF5 Polypropylene, 50% Calcium Carbonate Filled
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: UV Stabilized; Injection molding grade.

Applications: Commonly used as a concentrate. High flow for thin wall parts requiring long-flow. Toys, small appliances, outdoor furniture.

Data provided by Washington Penn Plastic Co., Inc.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.34 g/cc0.0484 lb/in³ASTM D792
Melt Flow 12 - 16 g/10 min12 - 16 g/10 minCond L; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.0 MPa3190 psiASTM D638
Flexural Yield Strength 41.0 MPa5950 psiASTM D790
Flexural Modulus 3.00 GPa435 ksiTangent; ASTM D790
Gardner Impact 14.5 J10.7 ft-lbASTM D3029

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Washington Penn Homopolymer Polypropylene 50% Calcium Carbonate Filled
Washington Penn Medium Impact Copolymer 50% Calcium Carbonate Filled
Adell EZ-18 Homopolymer Polypropylene, 40% Calcium Carbonate Filled
Abatron WoodEpox® Wood Replacement Compound
Abatron LiquidWood® Deep Penetrating Wood Consolidant

PWPP07 / 72790

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.