MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ovation Polymers OPTRENE 20GF Polypropylene, 20% Glass Reinforced
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Properties of chemically coupled glass reinforced (20%) polypropylene with high strength and HDT.

*All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Variations within normal tolerances are possible for various types of colors and functional properties like UV resistance.

Information provided by Ovation Polymers

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.033 g/ccASTM D792
Linear Mold Shrinkage 0.0024 - 0.0030 cm/cm
@Thickness 3.17 mm
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm
@Thickness 3.17 mm
Melt Index of Compound 14 - 16 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 68.0 MPa50 mm/min; ASTM D638
Elongation at Break 5.0 %50 mm/min; ASTM D638
Tensile Modulus 2.10 GPa50 mm/min; ASTM D638
Flexural Yield Strength 87.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.50 GPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 69.4 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 144 °C
@Thickness 3.20 mm
unannealed; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ovation Polymers SOFTAPLAS™ S 75A Thermoplastic Elastomer
Ovation Polymers OPTRENE 30GF Polypropylene, 30% Glass Reinforced
Ovation Polymers Nima™ NH PC151 Polycarbonate
Ovation Polymers Opnyl OP66GF13 Nylon 66, 13% Glass Reinforced
Ovation Polymers Opnyl OP66GF15 Nylon 66, 14% Glass Reinforced

POVAT089 / 55801

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.