MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Multibase Multi-Pro® 4006 T H BLK 40% Talc Content Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene with 40% Talc Filler

Material Notes: Multi-Pro 4002 T H is a talc reinforced polypropylene compound with excellent stiffness at medium impact resistance. Its heat resistance is improved over natural and can resist 150°C for 750 hours in an accelerated oven aging test. This product meets CMP PP 010 specifications.

Data provided by Multibase.

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.24 g/ccASTM D792-91
Linear Mold Shrinkage 0.0080 cm/cmASTM D955-89
Melt Flow 5.0 g/10 min(Condition L) ASTM D-1238-94a
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 7710 sec; ASTM D-2240-95
Tensile Strength, Ultimate 30.3 MPaASTM D638-95
Elongation at Break 25 %ASTM D638-95
Flexural Modulus 3.276 GPaSecant 20% strain; ASTM D-790-95
Izod Impact, Notched 0.320 J/cmASTM D256-93a
Gardner Impact 0.700 JASTM D5420-93
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 118 °CASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 64.0 °CASTM D648-95

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Adell RA-18 Copolymer Polypropylene, 40% Talc Filled
Inno-Comp INNOPOL® CS 1-6140 N 40% Talc-Filled Polypropylene Homopolymer
Adell RQ-18 Copolymer Polypropylene, 40% Mica Reinforced
A. Schulman Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled
A. Schulman Fiberfil® M-1812 Polypropylene Homopolymer, 45% Talc Filled

PLA252 / 49649

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.