MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Kraiburg TPE THERMOLAST® K TF3BNA Thermoplastic Elastomer (FC/AP Series) Adhesion to PP
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes: The FC/AP series is a material solution for everyday life applications with regulatory requirements for the Asia Pacific market. It is available in natural or translucent colors. The series is characterized by its PP adhesion.

Processing Method: Injection Molding

Color / RAL DESIGN:

  • Natural
  • Translucent
Typical applications:
  • Seals for housings
  • Function and design elements
  • Grip applications
  • Household articles
  • Razors
  • Toys
  • Packaging
  • Toothbrushes
Material advantages:
  • Adhesion to PP
  • Colorable
  • Optimized mechanical properties
  • Optimized flow properties
  • Halogen-free (according to IEC 61249-2-21)
  • In-process recycling possible
  • Non-sticky surface

Information provided by Kraiburg TPE

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.11 g/ccDIN EN ISO 1183-1
Storage Temperature 15.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 29DIN ISO 48-4
Tensile Strength 2.50 MPa200 mm/min; DIN 53504/ISO 37
Elongation at Break 650 %200 mm/min; DIN 53504/ISO 37
Tear Strength 10.0 kN/mISO 34-1 Method B (b)
 
Descriptive Properties
ColorNatural

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKRAIA8175 / 308839

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.