MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Solvay ANTAROX® BL 225 Surfactant
Categories: Fluid

Material Notes: Description: Biodegradable linear alcohol EO/PO. Low foaming non-ionic with excellent hard surface detergency combined to wetting properties. Soluble in water and most organic solvents except paraffinics. Stable in acidic and alkaline solutions. Can be used as a rinse aid forcommercial diswashing or mischellaneous industrial applications. Compliant with the EU's detergent biodegradability regulation.

Chemical Name: ETHOXYLATED PROPOXYLATED C8-C10 ALCOHOLS

CAS: 68603-25-8; 7732-18-5

Available in: Asia Pacific, Europe, Latin America and North America

Applications: ANTAROX© BL-225 is a non-ionic surfactant with excellent hard surface detergency combined with wetting properties at low foam levels (up to 50ºC). ANTAROX© BL-225 is stable to acids and soluble in water and most organic solvents except paraffinics. ANTAROX© BL-225 may be used as a rinse aid for commercial dishwashing (detergency), textiles (wetting detergency), and in metal treatment applications.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.990 g/cc
Viscosity 40 cP
 
Thermal PropertiesOriginal ValueComments
Boiling Point 200 °C
Flash Point 190 °CCleveland Open Cup
 
Optical PropertiesOriginal ValueComments
Gardner Color Number <= 3.0RP-0138
 
Processing PropertiesOriginal ValueComments
Shelf Life 24.0 Month
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.50 %Karl Fisher; RP-0327
 
Descriptive Properties
AppearanceClear to slightly hazy liquidRP-0064
Cloud point25-29°C1% Solution, RP-0124
Ionic ChargeNonionic
Neutralization Number<0.5 mg KOH/mgpH 7, RP-0343

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Solvay ANTAROX® BL 480 Surfactant
Solvay ANTAROX® BL 330 Surfactant
Solvay ANTAROX® L 61 Surfactant
Solvay ANTAROX® L 62 Surfactant
Solvay ANTAROX® L 62 LF Surfactant

WRHOD075 / 137306

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.