MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BP Amoco Acclear® 6219 Homopolymer Polypropylene, High Clarity Grade  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: Suggested fabrication methods: Sheet extrusion; Thermoforming

Features: High clarity, High heat resistance, Good melt strength/flow balance

Typical applications: Rigid packaging

Complies with FDA specification, Title 21, CFR 177.1520.

Typical property data below from injection molded samples.

Key Words: High Clarity, High Heat Resistance, Good Melt Strength/Flow Balance
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.886 - 0.926 g/ccASTM D1505
Water Absorption <= 0.010 %24 hours; ASTM D570
Linear Mold Shrinkage 0.010 - 0.025 cm/cmASTM D955
Melt Flow 2.2 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 39.0 MPaASTM D638
Flexural Modulus 1.65 GPaASTM D790A
Izod Impact, Notched 0.320 J/cm
@Diameter 3.17 mm
bar; ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 116 °CASTM D648
 
Optical PropertiesOriginal ValueComments
Haze 23 %
@Thickness 1.27 mm
plaque; ASTM D1003
Transmission, Visible 90 %clear; thickness not quantified
 
Compliance PropertiesOriginal ValueComments
FDA Yes

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Conditioned)
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
BASF Ultramid® 8233G HS 33% Glass Filled PA6 (Dry)
BASF Ultramid® 1000-11 NF2001 PA66 (Conditioned)
Covestro Makroblend® UT305 PC/PET Blend

PBPP00 / 27641

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.