MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M44 Moldable
Categories: Ceramic; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or spread into thin sections as coating and separating mediums.

APPLICATION: THERMOSEAL® FIBERPAK® MOLDABLES are applied with the fingers, towels, spatulas, or from caulking guns. Gloves should be worn when hand applying. THERMOSEAL® FIBERPAK® MOLDABLES are easily formed to any contour or readily pressed into cracks and smoothed out. Water wet the tool to facilitate smoothing and contouring. Drying consists of removing the liquid portion of the mix usually by use of an external heat source at 220-200ºF • 95-150ºC for approximately six hours per inch of thickness.

USES:

  • Trough linings for molten metal transfer
  • High temperature sealing and coating
  • Light weight refractory shape manufacture
  • Trough coating and patching
  • Furnace Patching

PACKAGING:

  • 11 oz. Caulking tubes
  • 32 oz. Caulking tubes
  • One Gallon Bucket
  • 5 Gallon Buckets
  • 55 Gallon Drums

Information provided by Mid-Mountain Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 54.0 lb/ft³Fired Density at 2300°F
 100 lb/ft³Wet Density
 57.0 lb/ft³
@Temperature 121 °C
Dry Density
Solids Content 55 %Wet
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 2300 °FUse Limit
Shrinkage -6.00 %
@Temperature 1260 °C
 
Descriptive Properties
Alumina19%fired
AppearanceSticky Putty
ColorWhite
DescriptionMoldable
Silica81%fired

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M22 Moldable
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M33 Moldable

CMID47 / 1551

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.