MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow BETAMATE™ 1045 Epoxy  (discontinued **)
Categories: Polymer; Thermoset; Epoxy

Material Notes: BETAMATE™ 1045 is a one component, epoxy based adhesive especially developed for the body shop. The product has the following properties:
  • Good rheology performance (Wash-out resistant, excellent after gelling)
  • Readily pumped at moderate temperatures
  • Excellent adhesion to automotive steels, including coated steels and pretreated aluminum
  • Resistant to degradation and substrate corrosion on environmental aging
  • Compatible with electro-coat paint process in uncured state

Information provided by Dow

BETAMATE™ is now a DuPont product line, but this specific product was discontinued while BETAMATE™ was a Dow product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 - 1.35 g/cc
Solids Content >= 99 %
Viscosity 900000 cP
@Shear Rate 1 1/s,
Temperature 40.0 °C
cone/plate
 2.50e+6 cP
@Shear Rate 1 1/s,
Temperature 23.0 °C
cone/plate
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 30.0 MPaISO 527-1
Elongation at Break 3.5 %ISO 527-1
Modulus of Elasticity 2.50 GPaISO 527-1
Adhesive Bond Strength 13.6 MPa
@Thickness 0.750 mm
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203); EN 1465
 20.9 MPa
@Thickness 1.50 mm
Lap Shear (25 x 10 x 0.2 mm) (CRS St 1203); EN 1465
Peel Strength 3.40 kN/mT-Peel (CRS St 1203, 0.5mm)
 7.00 kN/mImpact Peel
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 302 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 30.0 min
@Temperature 180 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Betamate™ 1496V Epoxy Adhesive, Body Shop Grade
DuPont BETAMATE™ 73345G Epoxy
DuPont Mobility and Materials Betamate™ 5103-2 Epoxy Adhesive, Body Shop Grade
Dow BETAMATE™ 7000/7050 L Epoxy
Dow CYRACURE™ UVR-6107 Cycloaliphatic Epoxide

PZDOW1003 / 30207

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.