MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Vectra® A420 Liquid Crystal Polymer (LCP), Glass/Mineral/Graphite Filled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes:

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.89 g/ccISO 1183
Water Absorption 0.020 %Immersion to equilibrium; ISO 62
Moisture Absorption at Equilibrium 0.020 %ISO 62
Linear Mold Shrinkage 0.0010 cm/cm
Linear Mold Shrinkage, Transverse 0.0020 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 79ISO 2039-2
Tensile Strength, Ultimate 145 MPaISO 527
Elongation at Break 1.4 %IEC 527
Tensile Modulus 22.0 GPaISO 527
Flexural Strength 200 MPaISO 178
Flexural Modulus 20.0 GPaISO 178
Compressive Strength 131 MPa1% Deflection, ISO 604
Compressive Modulus 21.5 GPaISO 604
Izod Impact, Notched (ISO) 0.600 J/cm²ISO 180/1A
Charpy Impact, Notched 0.800 J/cm²ISO 179
Coefficient of Friction, Dynamic 0.17vs. steel; ASTM D1984
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+12 ohm-cmIEC 93
Surface Resistance 1.00e+16 ohmIEC 93
Dielectric Constant 5.9
@Frequency 1e+7 Hz
 6.7
@Frequency 1000 Hz
IEC 250
Dissipation Factor 0.020
@Frequency 1000 Hz
IEC 250
 0.020
@Frequency 1e+7 Hz
Arc Resistance 180 sec
Comparative Tracking Index 250 VIEC 112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 11.0 µm/m-°C
@Temperature -50.0 - 200 °C
CTE, linear, Transverse to Flow 51.0 µm/m-°C
@Temperature -50.0 - 200 °C
Melting Point 280 °CISO 3146
Maximum Service Temperature, Air 130 °CGeneric Rating for Vectra LCP
Deflection Temperature at 1.8 MPa (264 psi) 230 °CISO 75/A
Vicat Softening Point 238 °CASTM D1525
UL RTI, Electrical 130 °CGeneric Rating for Vectra LCP
UL RTI, Mechanical with Impact 130 °CGeneric Rating for Vectra LCP
Flammability, UL94 V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Vectra® A440 Liquid Crystal Polymer (LCP), Glass/PTFE Filled
Celanese VECTRA S135 LCP, 35% Glass Reinforced
Celanese Vectra® A422 Liquid Crystal Polymer (LCP), Glass/Graphite Filled
Aluminum 5052-H32
Celanese VECTRA E820i LCP, 40% Specialty

PHCU92 / 45832

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.