MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

(Viewing data as-entered. Click here to return)
Master Bond EP40Med Two component, room temperature curing epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: Key Features:
  • Convenient handling
  • Long open time
  • Good bond strength in shear and peel
  • Exceptional adhesion to polycarbonates and acrylics
Master Bond EP40Med is a two part, room temperature curing epoxy for bonding, sealing, coating and encapsulating. This low to moderate viscosity system has a forgiving 1 to 1 mix ratio by weight or volume. It is formulated to cure readily at ambient temperatures or more rapidly at elevated temperatures. The optimum curing schedule is overnight at room temperature followed by 2-3 hours at 120°F to 150°F. EP40Med is 100% reactive and contains no solvents or diluents. EP40Med bonds well to a variety of substrates including metals, ceramics, composites and plastics. Its forte is adhesion to engineered plastics such as polycarbonates and acrylics. EP40Med is inherently tough and can withstand intense thermal cycling and shock. EP40Med cures firm, but is inherently tough and flexible. It can withstand intense thermal cycling and shock. Also, it is a reliable electrical insulator. This combined with its low viscosity and low exotherm enables it to be utilized as a potting and encapsulating system. It can resist various kinds of sterilization including EtO, gamma, and other liquid disinfectants. The color of Part A is clear and Part B is amber. The service temperature range is -80°F to +250°F. EP40Med is a highly desirable system for medical device manufacturing and repair. It can be used in both disposable and reusable instruments. It is most desirable in applications where toughness and flexibility along with good structural adhesive properties are needed.

Product Advantages:

  • One to one mix ratio by weight or volume
  • Relatively long open time
  • Good lap shear and exceptionally high peel strength
  • Very high elongation
  • Special affinity for polycarbonates and acrylics
  • Meets the ISO 10993-5 specification

Information provided by Master Bond Inc.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Viscosity 6000 - 8000 cPPart B
 9000 - 16000 cPPart A
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50 - 60
Tensile Strength 2000 - 3000 psi
Elongation at Break 80 - 90 %
Tensile Modulus 25000 - 50000 psi
Adhesive Bond Strength 1600 - 1800 psiTensile Lap Shear; Al/Al
Peel Strength 60.0 - 80.0 plisteel to steel
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cm
Dielectric Constant 4.1
@Frequency 60 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 50.0 - 60.0 µm/m-°C
Maximum Service Temperature, Air 121 °C
Minimum Service Temperature, Air -62.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 2.00 - 3.00 hour
@Temperature 48.9 - 65.6 °C
Optimum cure schedule: overnight at 75°F, plus 2-3 hours at 120-150°F
 48.0 - 72.0 hour
@Temperature 23.9 °C
Option
Working Life 120 - 150 min
@Temperature 23.9 °C
After mixing, 100 gram batch
Shelf Life 6.00 Month
 
Descriptive Properties
Mixing ratio1:1 by weight or volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM611 / 249007

USP Class VI adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.