MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LG Chemical NBR 6830 High Acrylonitrile Polymer  (discontinued **)
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Description: NBR 6830 is a copolymer of butadiene and acrylonitrile manufactured by advanced emulsion polymerization technology of Goodyear and LG Chem. NBR 6830 is a non staining, medium low mooney, and medium high acrylonitrile polymer designed for easy processing, high productivity and excellent elastic properties. NBR 6830 offers very low mold fouling, fast cure, and high resilience. NBR 6830 is low mooney version of NBR 6840

Applications: NBR 6830 is recommended to use in wide range of general purpose applications including injection molded o-rings, calendared belting, extruded hose and sponge.

CAS No: 9003-18-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.980 g/cc
Volatiles 0.30 %
Mooney Viscosity 31
@Temperature 100 °C
ML 1+4
Ash <= 1.0 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 27.0 MPa
@Treatment Temp. 145 °C,
Time 2990 sec
cured; ASTM D412
Elongation at Break 500 %
@Treatment Temp. 145 °C,
Time 2990 sec
cured; ASTM D412
300% Modulus 145 kg(f)/cm²
@Treatment Temp. 145 °C,
Time 2990 sec
cured; ASTM D412
 
Descriptive Properties
Bound AN Content (%)34
ColorLight Tan
ComponentsHAF (IRB#7)40 phr, ASTM D3187
 NBR 6830100 phr, ASTM D3187
 Stearic Acid1 phr, ASTM D3187
 Sulfur1.5 phr, ASTM D3187
 TBBS0.7 phr, ASTM D3187
 ZnO3 phr, ASTM D3187

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Plenco 2000 Phenolic, Granular, Injection Molded
LG Chemical NBR 6840 High Acrylonitrile Polymer
LG Chemical NBR 6280 High Acrylonitrile Polymer
LG Chemical NBR 6260 High Acrylonitrile Polymer
LG Chemical NBR 6250 High Acrylonitrile Polymer

PLAY736 / 148746

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.