MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 6035-55A Specialty Thermoplastic Elastomer, Clear
Categories: Polymer; Thermoplastic; Elastomer, TPE

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D 792
Linear Mold Shrinkage 0.015 - 0.045 cm/cm
@Thickness 3.17 mm
0.015 - 0.045 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 555510 s delay; ASTM D 2240
Tensile Strength at Break 9.65 MPa
@Thickness 3.17 mm
1400 psi
@Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
Tensile Stress at Strain 1.38 MPa
@Strain 100 %,
Thickness 3.17 mm
200 psi
@Strain 100 %,
Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
Elongation at Break 720 %
@Thickness 3.17 mm
720 %
@Thickness 0.125 in
Die C; 20 in/min (500 mm/min); ASTM D412
Tear Strength 38.6 kN/m220 pliDie C; ASTM D 624
Compression Set 25 %
@Temperature 23.0 °C,
Time 79200 sec
25 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; Type 2; ASTM D 395
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Processing PropertiesMetricEnglishComments
Melt Temperature 182 - 232 °C360 - 450 °F
Mold Temperature 15.6 - 65.6 °C60.0 - 150 °F
Drying Temperature 51.7 °C125 °F
Dry Time 2 - 4 hour2 - 4 hour
Dew Point <= -17.8 °C<= 0.000 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow Silastic® Q7-4750 BIOMEDICAL GRADE ETR ELASTOMER, KIT
Momentive Performance Materials Addisil™ 1050 E Industrial Extrusion Heat Cured Rubber
Wacker Elastosil® R plus 4000/50 Silicone Rubber
NuSil MED-2245 Two-Part Standard High Consistency Elastomers - Unrestricted Medical Use
Multibase C6-135 Dow-Corning Class VI Elastomer

PQZWA5547 / 92041

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.