MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Sumitomo Bakelite North America 2008A Glass Reinforced Hardware Grade Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Molded, Glass Fiber Filler; Filled/Reinforced Thermoset

Material Notes: Epoxy is the premier material for military firewall connectors.

Information provided by Sumitomo Bakelite North America, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.85 g/ccASTM D792
Water Absorption 0.20 %48 hours, 50°C. ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cmCompression Molding. ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 72
Tensile Strength, Ultimate 62.0 MPaASTM D638
Flexural Yield Strength 124 MPaASTM D790
Flexural Modulus 15.2 GPaASTM D790
Compressive Yield Strength 207 MPaASTM D695
Izod Impact, Notched 0.350 J/cmASTM D256A
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.0Wet; ASTM D150
Dielectric Strength 12.0 kV/mmWet, short term. ASTM D149
Dissipation Factor 0.019
@Frequency 1e+6 Hz
Wet; ASTM D150
Arc Resistance 180 secASTM D495
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 37.0 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Thermal Conductivity 0.691 W/m-KASTM F433
Deflection Temperature at 1.8 MPa (264 psi) 260 °CASTM D648A
Oxygen Index 50 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Mold Temperature 143 - 177 °Ccompression/transfer molding.
 174 - 182 °Cinjection molding.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sumitomo Bakelite North America 4064 Mineral Filled Electrical Encapsulation Grade Epoxy
Sumitomo Bakelite SUMIMAC® ECR-9250K Epoxy Resin
Sumitomo Bakelite SUMIMAC® ECR-9125K Epoxy Resin
Sumitomo Bakelite SUMIMAC® ECR-2222K + ECH-222G Epoxy Resin
Sumitomo Bakelite North America RX® 865M Novolac Phenolic

PROG64 / 66275

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.