MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Celanese Celstran® PEHD-GF60-01 PE-HD, 60% Glass Reinforced
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Glass fiber Filled

Material Notes: 58% long strand glass fiber reinforced high density polyethylene

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccASTM D792
Density 1.50 g/ccISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 91.0 MPa5mm/min; ISO 527-2/1A
 16400 psiASTM D638
 7100 psi
@Temperature 93.3 °C
ASTM D638
 23400 psi
@Temperature -40.0 °C
ASTM D638
Elongation at Break 1.38 %5mm/min; ISO 527-2/1A
 1.5 %ASTM D638
Tensile Modulus 10500 MPa50mm/min; ISO 527-2/1A
 1.97e+6 psiASTM D638
 1.04e+6 psi
@Temperature 93.3 °C
ASTM D638
 2.21e+6 psi
@Temperature -40.0 °C
ASTM D638
Flexural Strength 160 MPaISO 178
 25800 psiASTM D790
 8900 psi
@Temperature 93.3 °C
ASTM D790
 31200 psi
@Temperature -40.0 °C
ASTM D790
Flexural Modulus 11700 MPaISO 178
 1.58e+6 psiASTM D790
 827000 psi
@Temperature 93.3 °C
ASTM D790
 2.04e+6 psi
@Temperature -40.0 °C
ASTM D790
Izod Impact, Notched 7.00 ft-lb/inASTM D256
 4.00 ft-lb/in
@Temperature 93.3 °C
ASTM D256
 8.60 ft-lb/in
@Temperature -40.0 °C
ASTM D256
Charpy Impact, Notched 30.0 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 250 °FASTM D648
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 70.0 °Ccavity
Feed Temperature 20.0 - 50.0 °C
Zone 1 200 - 210 °C
Zone 2 210 - 220 °C
Zone 3 220 - 230 °C
Zone 4 230 - 240 °C
Die Temperature 230 - 240 °C
Melt Temperature 230 - 240 °C
Drying Temperature 90.0 - 100 °C
Dry Time 2.00 hour
Moisture Content <= 0.20 %
 
Descriptive Properties
Injection moldingYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Celstran® PEHD-GF40-01 PE-HD, 40% Glass Reinforced
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
A. Schulman Matrixx FPE3A40 40% Glass Reinforced Polyethylene
RTP Company RTP 700 GB 30  High Density Polyethylene (HDPE) Glass Bead 30%
LATI Latene® HD 2 G/20 20% Glass Fiber Reinforced High Density Polyethylene (HDPE)

PHCQ193 / 178648

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.