MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Melos FM 972 Flame-retardant bedding compounds for XLPE insulation and HFFR sheathing
Categories: Polymer; Thermoplastic

Material Notes: Flame-retardant bedding compounds for XLPE insulation and HFFR sheathing.

Compound class: Bedding compound

Based on: EPR

Characteristics: Halogen free flame retardant

Application examples: Insulation
2 YI 1 – 5; PE; acc. DIN / VDE 0207 part 2
9 YI 1; PP; acc. DIN / VDE 0207 part 7
YI 1 – 5; PVC; acc. DIN / VDE 0207 part 20

Application examples: Sheathing
HM 4 – 2; HFFR; acc. DIN / VDE 0207 part 24
2 YM 3; HDPE; acc. DIN / VDE 0207 part 3

Typical applications: Bedding compound for cables and wire with max. 90°C operating temperature at conductor.

Features: For tandem process; Flame retardant; Halogen-free

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.74 g/ccpressed plaques, 100°C / 5 min.; DIN EN ISO 1183-1A
pH >= 4.3Corrosivity, pressed plaques, 100°C / 5 min.; IEC 60754-2
Mooney Viscosity 28
@Temperature 100 °C
ML (1+4); DIN ISO 289-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 75pressed plaques, 100°C / 5 min.; DIN ISO 7619-1
Tensile Strength >= 0.500 MPapressed plaques, 105°C / 5 min.; IEC 60811-501
Elongation at Break >= 20 %pressed plaques, 105°C / 5 min.; IEC 60811-501
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+12 ohm-cm
@Temperature 27.0 °C
VDE 0472 Part 503
Surface Resistance >= 1.00e+9 ohm
@Temperature 23.0 °C
VDE 0472 Part 502
 
Processing PropertiesOriginal ValueComments
Processing Temperature 80.0 - 90.0 °CTool
 80.0 - 90.0 °CMaximum mass temperature
Zone 1 60.0 - 70.0 °C
Zone 2 65.0 - 75.0 °C
Zone 3 65.0 - 75.0 °C
Zone 4 70.0 - 80.0 °C
Adapter Temperature 70.0 - 80.0 °C
Head Temperature 75.0 - 85.0 °C
Shelf Life 12.0 Month
 
Component Elements PropertiesOriginal ValueComments
Loss on Ignition(%) 50 %pressed plaques, 100°C / 5 min.; ASTM D 2863 A
 
Descriptive Properties
Conductivity=100 µS/mmpressed plaques, 100°C / 5 min., IEC 60754-2
Main burning properties7900 kJ/kgCaloric Value Hu, DIN 51900-2
Screw60-70°C
Temperature index290°CISO 4589-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMELOS073 / 296180

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.