MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Flame Retardant adhesives

(Viewing data as-entered. Click here to return)
Cookson Group Plaskon® CMU-870-2B Molded Underfill Compound for Flip Chip BGAs and CSPs  (discontinued **)
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Molding Compound

Material Notes: This material is an epoxy Molded Underfill compound developed for transfer mold equipment to underfill, and overmold if needed, Flip Chip in Package (FC-BGA and FC CSP) in one step. It offers high productivity with an automated, simple, robust and fast process compared to liquid encapsulation. Higher reliability is demonstrated with the material’s higher Tg, lower CTE, no particle segregation or settling and longer outlife compared to liquid encapsulants. PLASKON CMU Series is the total molded underfill solution for Flip Chip in Package.

Features:

  • Higher productivity
  • Higher Tg
  • Higher reliability
  • Lower warpage
  • Lower CTE
  • Lower cost of ownership
  • Minimum 220°C reflow
  • Minimum JEDEC Level 3

Applications:

Plaskon CMU-870-2B Molded Underfill is suitable for high volume underfill and overmold protection of Flip Chip BGA and CSP packages. It is suitable for stack die packages using a combination of wirebonded and flip chip dies wh

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.89 g/cc
Viscosity 5000 cP
@Temperature 175 °C
Shimadzu Viscosity, 1000 psi
Linear Mold Shrinkage 0.00050 cm/cm
Spiral Flow 125 cmat 175°C and 1000 psi
Ash 80 %
Storage Temperature <= 5.00 °CRecommended
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85Cull hot
Flexural Strength 12090 psi
 4978.2 psi
@Temperature 215 °C
Flexural Modulus 2.560e+6 psi
 853400 psi
@Temperature 215 °C
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 4.50e+15 ohm-cm
Dielectric Constant 3.13
@Frequency 1000 Hz
Dielectric Strength >= 800 V/mil
Dissipation Factor 0.0017
@Frequency 1000 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.0 µm/m-°C
@Temperature 20.0 °C
Alpha 1
 55.0 µm/m-°C
@Temperature 20.0 °C
Alpha 2
Thermal Conductivity 0.750 W/m-K
Glass Transition Temp, Tg 195 °C
Flammability, UL94 V-0
@Thickness 3.17 mm
 
Processing PropertiesOriginal ValueComments
Mold Temperature 165 - 170 °C
Back Pressure 500 - 900 psi
Cure Time 100 - 200 secIn mold
Gel Time 0.233 minRam follower, at 175°C and 1000 psi
Shelf Life 0.0670 Monthat 35°C, <40% loss of spiral flow
 0.167 Monthat 21°C, <40% loss of spiral flow
 24.0 Monthat 5°C, <40% loss of spiral flow
 
Descriptive Properties
Hydrolyzable Halides<1 ppm
Preform Temperature80-85°C
Transfer Time6-15 seconds

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Epoxy Molding Compound
Cookson Group Plaskon® LS-16 Low Stress Epoxy Molding Compound
Cookson Group Plaskon® CMU-870-2C Molded Underfill Compound for Flip Chip BGAs and CSPs
Cookson Group Plaskon® CMU-870-2A Molded Underfill Compound for Flip Chip BGAs and CSPs
Cookson Group Plaskon® AMC-2RC Low Stress Epoxy Molding Compound

PPLASK034 / 56324

Flame Retardant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.